where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

ZETEC, Inc.
Zetec is a global leader in nondestructive testing (NDT) solutions for the critical inspection needs of industries the world counts on every day, ...
658 views
Technical Discussions
Hanurajie Baskan
Teacher, NDT Instructor
National Nuclear Energy Agency, Japan, Joined Oct 1999, 1

Hanurajie Baskan

Teacher, NDT Instructor
National Nuclear Energy Agency,
Japan,
Joined Oct 1999
1
08:44 Mar-13-2003
UT for thin material

Dear Everybody,
I'd like to ask to ndt forum about my new specimen TiNi (as actuator). What kind NDT method should I use for this one?. The thickness is 130 micro after rolling. Is there probability by ultrasonic, what kind method of UT?. I was trying by UT immersion 35 MHz focus tranducer, but really unsatisfied. Is there anybody can suggest to me.
Thank you in advance.
Best regard

Baskan


 
 Reply 
 
Kris Van de Rostyne
Kris Van de Rostyne
09:17 Mar-13-2003
Re: UT for thin material
Hello,
One possible solution to increase the bandwidth could be to use laser-ultrasonics. In this method, the ultrasonic waves are generated by the thermo-elastic expansion caused by the absorption of an incident laser pulse. The shorter the pulse-duration, the higher the bandwidth and resolution (but unfortunately, the higher the price I am afraid). For your application, a laser producing pulses of a few nanoseconds (e.g. Nd:YAG) should probably be convenient. Do you want to use UT for defect detection or for characterisation of properties?
Greetings,
Kris

: Dear Everybody,
: I'd like to ask to ndt forum about my new specimen TiNi (as actuator). What kind NDT method should I use for this one?. The thickness is 130 micro after rolling. Is there probability by ultrasonic, what kind method of UT?. I was trying by UT immersion 35 MHz focus tranducer, but really unsatisfied. Is there anybody can suggest to me.
: Thank you in advance.
: Best regard
.
: Baskan
.



 
 Reply 
 
C. Valdecantos
Engineering
MTORRES, Ing., Spain, Joined May 2001, 9

C. Valdecantos

Engineering
MTORRES, Ing.,
Spain,
Joined May 2001
9
01:56 Mar-13-2003
Re: UT for thin material
Depending on what are you looking for, some other ndt technique may be of use. For example, if the problem is to measure the thickness, Eddy Current may be the best, although this (Ti base?) alloy will probably show a very low conductivity. EC will also provide information (or even positive indication) on other parameters like cracks, inhomogeneities, laminar defects.

If EC is not suitable, perhaps thermografic analysis would be of use. In this case, the (supposed)low thermal conductivity of the material will help.


 
 Reply 
 

Product Spotlight

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Research and Applications Development For NDT

The Research and Applications Development (RAD) group is a newly formed team within Acuren dedicat
...
ed to tackling challenging inspection problems. Our focus is the development of novel, field deployable, advanced inspection techniques for use in cases where standard NDT methods are ineffective. We don't wait for new innovations, we engineer them. From concept to commissioning.
>

Panther

M2M PANTHER is a phased-array equipment designed for both desktop and industrial applications, offer
...
ing unparalleled performance in a compact unit. It combines the speed required for industrial integrated Phased-Array Ultrasound (PAUT) solutions, with the most complete set of total focusing method (TFM) imaging techniques, making it the ultimate tool for R&D and procedure qualification.
>

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window