Technical Discussions
kavita
kavita
03:04 Jan-24-2003
some questions regarding impact echo

I have some questions regarding NDE and impact echo in particular, for concrete pipes.
1)Has ever been SASW (spectral analysis of surface waves) been used for evaluating the integrity of concrete pipe. Can anybody give me a case study?
2)I've read some where that SASW and impact echo are similar to some extent. to what extent are they similar and hpw are they different.
3)why are S-waves ignored in impact echo testing?

Thanx advance for your answers




 
 Reply 
 
kavita
kavita
00:01 Jan-25-2003
one more question
: I have some questions regarding NDE and impact echo in particular, for concrete pipes.
: 1)Has ever been SASW (spectral analysis of surface waves) been used for evaluating the integrity of concrete pipe. Can anybody give me a case study?
: 2)I've read some where that SASW and impact echo are similar to some extent. to what extent are they similar and hpw are they different.
: 3)why are S-waves ignored in impact echo testing?
. 4)what is the difference between impact-echo and impulse response. is it that in impulse response the stress wave is generated by a transmitter and in impact-echo that is done by mechanical impact.
: Thanx advance for your answers
.



 
 Reply 
 
Franc Buijsen
Franc Buijsen
03:09 Jan-25-2003
Re: some questions regarding impact echo
I advise you to contact a company called Andec in Toronto Canada, andec@andec.on.ca. They are very familiar with concrete testing using impact echo.

regards

Franc

: I have some questions regarding NDE and impact echo in particular, for concrete pipes.
: 1)Has ever been SASW (spectral analysis of surface waves) been used for evaluating the integrity of concrete pipe. Can anybody give me a case study?
: 2)I've read some where that SASW and impact echo are similar to some extent. to what extent are they similar and hpw are they different.
: 3)why are S-waves ignored in impact echo testing?
.
: Thanx advance for your answers
.



 
 Reply 
 
Christian Grosse
Teacher,
Technische Universität München, Germany, Joined Nov 2000, 12

Christian Grosse

Teacher,
Technische Universität München,
Germany,
Joined Nov 2000
12
02:42 Jan-31-2003
Re: some questions regarding impact echo
These are several interesting questions and a discussion could be
useful. I am not an expert in SASW, but maybe you can point to a proper
source of information.

Regarding question 3 I am not sure if I understand the benefit you
expect to get using S-waves additionally to P-waves. However, since the
impact usually used in impact-echo testing produces mainly compressional
waves, I would not expect S-waves to be very dominant. These problems
are now addressed by a collaborative research project in Germany (see
http://www.for384.uni-stuttgart.de/) using a combination of experiments
and simulations. The answer is: This is ongoing research.

If you understand impulse response as a technique generating stress
waves by ultrasound emitters, this could be a difference to impact-echo.
To generate high amplitude pulses usually piezo-electric emitters of the
resonant type are used. The idea of impact-echo is instead to use
broadband pulses (pulses with energy over a broader frequency band) to
detect "reverbations" caused by flaws in different depth. This is
another difference to most ultrasound impulse techniques. The amplitudes
generated by broadband piezo-electric emitters are usually too weak.

Christian Grosse


---------------------------------
: I have some questions regarding NDE and impact echo in particular, for concrete pipes.
: 1)Has ever been SASW (spectral analysis of surface waves) been used for evaluating the integrity of concrete pipe. Can anybody give me a case study?
: 2)I've read some where that SASW and impact echo are similar to some extent. to what extent are they similar and hpw are they different.
: 3)why are S-waves ignored in impact echo testing?
.
: Thanx advance for your answers
.



 
 Reply 
 
kavita
kavita
00:33 Feb-05-2003
Re: some questions regarding impact echo
Thank You Mr.Grosse!


 
 Reply 
 
WILLIAM A. WEBER
Director
IMPACT-ECHO INSTRUMENTS,LLC, USA, Joined Mar 2003, 2

WILLIAM A. WEBER

Director
IMPACT-ECHO INSTRUMENTS,LLC,
USA,
Joined Mar 2003
2
06:16 Mar-24-2003
Re: some questions regarding impact echo
: These are several interesting questions and a discussion could be
: useful. I am not an expert in SASW, but maybe you can point to a proper
: source of information.
.
: Regarding question 3 I am not sure if I understand the benefit you
: expect to get using S-waves additionally to P-waves. However, since the
: impact usually used in impact-echo testing produces mainly compressional
: waves, I would not expect S-waves to be very dominant. These problems
: are now addressed by a collaborative research project in Germany (see
: http://www.for384.uni-stuttgart.de/) using a combination of experiments
: and simulations. The answer is: This is ongoing research.
.
: If you understand impulse response as a technique generating stress
: waves by ultrasound emitters, this could be a difference to impact-echo.
: To generate high amplitude pulses usually piezo-electric emitters of the
: resonant type are used. The idea of impact-echo is instead to use
: broadband pulses (pulses with energy over a broader frequency band) to
: detect "reverbations" caused by flaws in different depth. This is
: another difference to most ultrasound impulse techniques. The amplitudes
: generated by broadband piezo-electric emitters are usually too weak.
.
: Christian Grosse
.
:
: ---------------------------------
: : I have some questions regarding NDE and impact echo in particular, for concrete pipes.
: : 1)Has ever been SASW (spectral analysis of surface waves) been used for evaluating the integrity of concrete pipe. Can anybody give me a case study?
: : 2)I've read some where that SASW and impact echo are similar to some extent. to what extent are they similar and hpw are they different.
: : 3)why are S-waves ignored in impact echo testing?
: .
: : Thanx advance for your answers
: .
.CHRISTIAN,

TAKE A LOOK AT OUR WEBSITE, WWW.IMPACT-ECHO.COM; IT HAS CASE HISTORIES AND LOTS OF INFO. WE ALSO SELL THE BOOK ON THE TOPIC WHICH WILL ANSWER ALL YOUR QUESTIONS. SORRY NOT TO REPLY SOONER, BUT I JUST SAW YOUR QUESTION.

BILL WEBER



 
 Reply 
 

Product Spotlight

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>