Chemical Composition of P18 steel according to ISO9328-4:1991

Does anybody knows the chemical composition of P18 steel plates according to ISO9328-4:1991?


    
 
 
mohamed saleh
mohamed saleh
07:55 May-25-2003
Re: Chemical Composition of P18 steel according to ISO9328-4:1991
: Does anybody knows the chemical composition of P18 steel plates according to ISO9328-4:1991?
.ASTM A325M



    
 
 
Tran Van Thap
Tran Van Thap
06:53 Jul-11-2005
Re: Chemical Composition of P18 steel according to ISO9328-4:1991
: : Does anybody knows the chemical composition of P18 steel plates according to ISO9328-4:1991?
: .ASTM A325M
.
Dear Sir/ Madam,
We are a company from Vietnam,
Now we are practicing alot of cutting equipments, so if you have a kind let we kmow :
-Description your P18 steel chemical composition.
-Price
-Method to buy.
Thanks and best regard!
Tran Van Thap.
Vice Director,
Applied Electricity - Mehanics and Informatics Company.
LeKatek Co.,Ltd
201 Nguyen Khang, Yen Hoa ward, Cau Giay Dist.,Hanoi, Vietnam.
Tel: +84 4 7848789.
Fax: +84 4 7848401.
Email: lekatek@vnn.vn



    
 
 
tranvanthap
tranvanthap
06:10 Jul-26-2006
Re: Chemical Composition of P18 steel according to ISO9328-4:1991
----------- Start Original Message -----------
: : : Does anybody knows the chemical composition of P18


    
 
 

Product Spotlight

Teletest Focus+

Teletest Focus+ electronics have superior capabilities than rivals on the market. Beyond the usual
...
test features, Focus+ has 24 transmit channels and 24 receive channels, with an additional on-board switching capabilities. The instrument's frequency range is 10–300 kHz.
>

Echomac® Small

Available with up to eight channels of electronics to detect and evaluate thickness, flaws and eccen
...
tricity, this UT tester is housed in a convenient, smaller cabinet. This instrument can be used in conjunction with bubbler or immersion tank systems, or with a test bench or in laboratory applications. The Echomac® Small is available in the FD4, FD6 or FD6A versions.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window