ULTRASONIC INSPECTION OF WOODEN UTILITY POLES

I am seeking information on inspecting wooden utility
poles to determine the "life remaining" and "quantity of
decay". Also, where equipment such as the "sylvatest" or
similar low frequency ultrasonic equipment may be
purchased? Thank you.


 
 Reply 
 
Risto Backman
Risto Backman
00:17 Dec-10-1999
Re: ULTRASONIC INSPECTION OF WOODEN UTILITY POLES

I am seeking information on inspecting wooden utility
Also, where equipment such as the "sylvatest" or
similar low frequency ultrasonic equipment may be
purchased? Thank you.

Actually, we are interested in more info. as well as any lab result has been gained from this machine.

Ofcourse we need yr quotation and delivery time.




 
 Reply 
 
Ahmed Mubarrazi
Ahmed Mubarrazi
03:50 May-02-2000
Re: ULTRASONIC INSPECTION OF WOODEN UTILITY POLES
: I am seeking information on inspecting wooden utility
: poles to determine the "life remaining" and "quantity of
: decay". Also, where equipment such as the "sylvatest" or
: similar low frequency ultrasonic equipment may be
: purchased? Thank you.




 
 Reply 
 
Jerry
Jerry
01:20 May-11-2000
Re: ULTRASONIC INSPECTION OF WOODEN UTILITY POLES
:Try Engineering Data Management (EDM) in Fort Collins, CO. Good luck.

I am seeking information on inspecting wooden utility
: poles to determine the "life remaining" and "quantity of
: decay". Also, where equipment such as the "sylvatest" or
: similar low frequency ultrasonic equipment may be
: purchased? Thank you.




 
 Reply 
 
Stephen Bracegirdle
Sales
OIS Engineering Ltd, United Kingdom, Joined Feb 2000, 5

Stephen Bracegirdle

Sales
OIS Engineering Ltd,
United Kingdom,
Joined Feb 2000
5
00:16 May-12-2000
Re: ULTRASONIC INSPECTION OF WOODEN UTILITY POLES
: I am seeking information on inspecting wooden utility
: poles to determine the "life remaining" and "quantity of
: decay". Also, where equipment such as the "sylvatest" or
: similar low frequency ultrasonic equipment may be
: purchased? Thank you.

OIS Engineering has a field portable scanning jig for inspecting utility poles using digital radiography with CT. For further info please email me at seb@oisel.co.uk




 
 Reply 
 

Product Spotlight

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window