ULTRASONIC INSPECTION OF WOODEN UTILITY POLES

I am seeking information on inspecting wooden utility
poles to determine the "life remaining" and "quantity of
decay". Also, where equipment such as the "sylvatest" or
similar low frequency ultrasonic equipment may be
purchased? Thank you.


 
 Reply 
 
Risto Backman
Risto Backman
00:17 Dec-10-1999
Re: ULTRASONIC INSPECTION OF WOODEN UTILITY POLES

I am seeking information on inspecting wooden utility
Also, where equipment such as the "sylvatest" or
similar low frequency ultrasonic equipment may be
purchased? Thank you.

Actually, we are interested in more info. as well as any lab result has been gained from this machine.

Ofcourse we need yr quotation and delivery time.




 
 Reply 
 
Ahmed Mubarrazi
Ahmed Mubarrazi
03:50 May-02-2000
Re: ULTRASONIC INSPECTION OF WOODEN UTILITY POLES
: I am seeking information on inspecting wooden utility
: poles to determine the "life remaining" and "quantity of
: decay". Also, where equipment such as the "sylvatest" or
: similar low frequency ultrasonic equipment may be
: purchased? Thank you.




 
 Reply 
 
Jerry
Jerry
01:20 May-11-2000
Re: ULTRASONIC INSPECTION OF WOODEN UTILITY POLES
:Try Engineering Data Management (EDM) in Fort Collins, CO. Good luck.

I am seeking information on inspecting wooden utility
: poles to determine the "life remaining" and "quantity of
: decay". Also, where equipment such as the "sylvatest" or
: similar low frequency ultrasonic equipment may be
: purchased? Thank you.




 
 Reply 
 
Stephen Bracegirdle
Sales
OIS Engineering Ltd, United Kingdom, Joined Feb 2000, 5

Stephen Bracegirdle

Sales
OIS Engineering Ltd,
United Kingdom,
Joined Feb 2000
5
00:16 May-12-2000
Re: ULTRASONIC INSPECTION OF WOODEN UTILITY POLES
: I am seeking information on inspecting wooden utility
: poles to determine the "life remaining" and "quantity of
: decay". Also, where equipment such as the "sylvatest" or
: similar low frequency ultrasonic equipment may be
: purchased? Thank you.

OIS Engineering has a field portable scanning jig for inspecting utility poles using digital radiography with CT. For further info please email me at seb@oisel.co.uk




 
 Reply 
 

Product Spotlight

GUL Subsea Solutions - Screeening & Monitoring

To inspect new and existing subsea lines, you need proven technology and experience. GUL offers it's
...
technology to solve this challenge: GUL Subsea and gMAT Transducer Rings.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window