02:12 Apr-24-2003
Special coating for impact detection on composites

HI all

I recently heard about a product in which I would be interested if I had more information about it. This product is a (transparent ?) coating that can be sprayed on a composite structure. If the structure is impacted, the coating would keep 'memory' of the impact and would reveal it under fringing or UV light.
This is of course a very interesting product for localisation of sub surface small imact damages on composites.

That's all i know about it, plus that it is already an operational product and is, from what i heard, used by ARDE. But I do not know anything about its name, the company that produces it, etc.
Does anybody here know more about such product ?

Thanks in advance



 
 Reply 
 
Joerg Schulze-Clewing
Joerg Schulze-Clewing
02:50 Apr-24-2003
Re: Special coating for impact detection on composites
Hi Pierre,

Maybe a good start would be to check out SPIE at:
www.spie.org

This organization deals a lot with imaging, coatings etc.

Another might be the Brinell Centre in Stockholm.

Good luck, Joerg.


 
 Reply 
 

Product Spotlight

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window