measuring thickness of coextruded plastic

I am trying to find a sound analytical technique to measure the thickness of a layer of co extruded crystallized plastic. Approximate total thickness of about 20-25ml , the top layer needing measured is around 5 to 10% of total.

Any info you can provide will be appreciated.


 
 Reply 
 
Dr. Patel
Dr. Patel
04:57 Apr-29-2003
Re: measuring thickness of coextruded plastic
: I am trying to find a sound analytical technique to measure the thickness of a layer of co extruded crystallized plastic. Approximate total thickness of about 20-25ml , the top layer needing measured is around 5 to 10% of total.
.
: Any info you can provide will be appreciated.
.
We have measured plastic thickness down to 100 micron with micron accuracy. The system can be used for on-line application. If you are interested please contact me at fallon@netcom.ca. We are using very simple pulse echo technique with broadband pulse of 50 MHz. Some error may occur due to nature of plastic where velocity of material may change.
Regards
Dr. Patel
Fallon Ultrasonics Inc
905-388-7853
Fax 905 387 5897


 
 Reply 
 
Neil Burleigh
Sales
Krautkramer Australia Pty Ltd, Australia, Joined Dec 2002, 158

Neil Burleigh

Sales
Krautkramer Australia Pty Ltd,
Australia,
Joined Dec 2002
158
05:29 May-08-2003
Re: measuring thickness of coextruded plastic
: : I am trying to find a sound analytical technique to measure the thickness of a layer of co extruded crystallized plastic. Approximate total thickness of about 20-25ml , the top layer needing measured is around 5 to 10% of total.
: .
: : Any info you can provide will be appreciated.
: .
: We have measured plastic thickness down to 100 micron with micron accuracy. The system can be used for on-line application. If you are interested please contact me at fallon@netcom.ca. We are using very simple pulse echo technique with broadband pulse of 50 MHz. Some error may occur due to nature of plastic where velocity of material may change.
: Regards
: Dr. Patel
: Fallon Ultrasonics Inc
: 905-388-7853
: Fax 905 387 5897
.
Some years ago I was involved in trying to measure the total wall thickness of co extruded plastic containers. The total thickness was about 2.0 - 2.5 mm which comprised of three layers with the centre layer being made from recycled plastic.Using ultrasonics, a digital caliper, we were not able to penetrate the full thickness and were only ever able to measure the first layer which was about 0.5mm thick. We used a 22MHz probe on a gauge type CL202P.
Therefore depending on the grain size of the crystalized plastic outer layer you should try using a shockwave probe in the frequency of 15 - 25 MHz plus a UFD high frequency capabilities or a Krautkramer thickness gauge from the CL range.
If all this doesn't work can you send a sample to us for trials.

Regards



 
 Reply 
 

Product Spotlight

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Research and Applications Development For NDT

The Research and Applications Development (RAD) group is a newly formed team within Acuren dedicat
...
ed to tackling challenging inspection problems. Our focus is the development of novel, field deployable, advanced inspection techniques for use in cases where standard NDT methods are ineffective. We don't wait for new innovations, we engineer them. From concept to commissioning.
>

AMIGO2

TSC Amigo2 - ACFM technology has developed a solid reputation for accurately detecting and sizing
...
surface-breaking cracks through paint and coatings. As the industry demands increased performance in speed, signal quality, and portability, it’s time for an evolution. It’s time for Amigo2.
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window