02:06 May-05-2003
Measuring Stainless overlay 309L, 347L, 317L,316 etc.

Hello from South Carolina!!! well, once a year I go out to you all for you opinons on the above subject. Is there a system out there that can measure the thickness of Austentic overlay(ferrite)0.8 to 7.8 and it will vary. The welding application can vary also, but it is mostly automated. The backing is SA 285C or 516-70 mild steel (pressure vessels)or SA210 boiler tubes.For UT, the Z's factor is only 2. For magnetic induction or eddy current, the ferrite is the problem. We still measure befor overlay and after. The thickness will range from 1mm to 12mm.

Thankyou
M.C. Macke.


 
 Reply 
 
Doug Breeze
Director, Consultant; R&D
Inspection Software Limited, United Kingdom, Joined May 2000, 20

Doug Breeze

Director, Consultant; R&D
Inspection Software Limited,
United Kingdom,
Joined May 2000
20
08:44 Jun-05-2003
Re: Measuring Stainless overlay 309L, 347L, 317L,316 etc.
In response to Mike Macke's question a few weeks ago Dinsley Devices and Inspection Software have recently installed an automated system to measure Inconel cladding in the bore of 125mm - 300mm carbon steel pipe. Cladding thickness 0mm - 10mm, +/- 0.1mm. Should be suitable for other similar materials.



 
 Reply 
 

Product Spotlight

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

GUL Subsea Solutions - Screeening & Monitoring

To inspect new and existing subsea lines, you need proven technology and experience. GUL offers it's
...
technology to solve this challenge: GUL Subsea and gMAT Transducer Rings.
>

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window