Koblenz aluminium residual stress ultrasonic measurement

Does any one know something about ultrasonic measurement of residual stress in Koblenz aluminium alloy company?

Thanks

 
 Reply 
 
Syed Ali
R & D,
Innerspec Technology, USA, Joined Oct 2009, 17

Syed Ali

R & D,
Innerspec Technology,
USA,
Joined Oct 2009
17
14:45 Oct-06-2014
Re: Koblenz aluminium residual stress ultrasonic measurement
In Reply to Wang Xiao at 08:14 Oct-05-2014 (Opening).

Residual Stress measurements can be measured using two zero degree shear horizontal waves in orthogonal orientation which provides a Birefringence (%age) parameter directly related to the stress. Emats can easily generate linearly polarized SH waves in Aluminum.

Innerspec Technologies Inc also represented in Chinal has a specific emat probe to measure residual stress using their portable Power Box-H instrument. Kindly consult Innerspec Technologies for more details.

 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

VeeScan AirCraft Wheel Inspection

The VEESCAN offers maximum flexibility, has a proven mechanical design and records of breakdown-fr
...
ee operation of over 365 days. Appealing to companies in the Aerospace industry, the VEESCAN is ideal for all wheel-testing environments. With a wide selection of probes, the VeeScan allows your wheel testing facility the flexibility to select the most compatible configurations with their workload.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window