Koblenz aluminium residual stress ultrasonic measurement

Does any one know something about ultrasonic measurement of residual stress in Koblenz aluminium alloy company?

Thanks

 
 Reply 
 
Syed Ali
R & D,
Innerspec Technology, USA, Joined Oct 2009, 17

Syed Ali

R & D,
Innerspec Technology,
USA,
Joined Oct 2009
17
14:45 Oct-06-2014
Re: Koblenz aluminium residual stress ultrasonic measurement
In Reply to Wang Xiao at 08:14 Oct-05-2014 (Opening).

Residual Stress measurements can be measured using two zero degree shear horizontal waves in orthogonal orientation which provides a Birefringence (%age) parameter directly related to the stress. Emats can easily generate linearly polarized SH waves in Aluminum.

Innerspec Technologies Inc also represented in Chinal has a specific emat probe to measure residual stress using their portable Power Box-H instrument. Kindly consult Innerspec Technologies for more details.

 
 Reply 
 

Product Spotlight

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>