Coating Thickness Measurement

Hi,

I am trying to find a device in order to obtain the thicknesses values of a Aluminium Coating over Nickel base substrate.

Can anybody help me?

Thanks in advanced


 
 Reply 
 
Doug Breeze
Director, Consultant; R&D
Inspection Software Limited, United Kingdom, Joined May 2000, 20

Doug Breeze

Director, Consultant; R&D
Inspection Software Limited,
United Kingdom,
Joined May 2000
20
00:19 Jun-06-2003
Re: Coating Thickness Measurement

Not sure if we can help but what thicknesses are involved? Presumably microns of Aluminium over mm of Nickle. What form does the Nickle take... wire, plate rod, foam, sinter, coating, etc?




 
 Reply 
 
Sergio
Sergio
02:08 Jun-06-2003
Re: Coating Thickness Measurement
The thickness goes from 0,015 to 0,075 mm.

The base material goes from 1 mm to 3 mm aprox.

Thanks


 
 Reply 
 
John Hansen
Director, - Eddy Current Technology
ETher NDE Ltd, United Kingdom, Joined Oct 1999, 73

John Hansen

Director, - Eddy Current Technology
ETher NDE Ltd,
United Kingdom,
Joined Oct 1999
73
04:44 Jun-06-2003
Re: Coating Thickness Measurement
Hi Sergio

Providing the aluminium is pure then this should be possible with an eddy current procedure.

My honest advice is that you should try Fischer Technology from Germany for an off the shelf solution http://www.helmut-fischer.de/ (a competitor of ours) first.

If this material is too thin for them then I feel that with one of our standard instruments (e.g. Phasec 2s www.phasec2.com) a procedure could be developed or possibly using our conductivity meter (AutoSigma 3000 http://www.hocking.com/as_3000.htm).

Regards
John Hansen
Industrial Product Manager
Hocking NDT Ltd.
e-mail Jhansen@hocking.com
web www.hocking.com
tel +44 (0) 1727 795509
fax +44 (0) 1727 795409



 
 Reply 
 
Doug Breeze
Director, Consultant; R&D
Inspection Software Limited, United Kingdom, Joined May 2000, 20

Doug Breeze

Director, Consultant; R&D
Inspection Software Limited,
United Kingdom,
Joined May 2000
20
05:34 Jun-06-2003
Re: Coating Thickness Measurement

John Hansen's advice is correct. There are several suppliers who should be able to supply hand-held gauges to measure Al on Ni economically... search on Google for 'Coating Thickness Guages' if necessary.

The task may get more unpredictable for Ni alloys and/or at changes in component section. If you need a computerised or automated system contact me separately.



 
 Reply 
 

Product Spotlight

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

SONOAIR - air-coupled Phased Array Ultrasonic Inspection System

For highly attenuating materials, the performance of the system is critical. The ultrasonic sensors,
...
the scanning area and the system settings should be flexibly adapted to the test task and the material. These high expectations are met with the new and modular testing system SONOAIR. With the world’s first air-coupled phased-array UT inspection system SONOAIR we developed a technology that works with up to 4 transmitter and receiver channels with freely configurable square wave burst transmitters as wells as low noise receiving amplifiers.
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window