Calibration Procedures for Immersion Ultrasound Testing

Hi all,

I am a researcher working on Ultrasound immersion testing of Aluminium parts.
I have a copy of the Australian Standard 2083-1981 -- Calibration Blocks and their methods of use in Ultrasonic Testing,
which explains basically about the ultrasound contact testing.

My question is whether there are any separate calibration standards for ultrasound immersion testing.
If so what are they.

Thank you,

Suresh Palanisamy



 
 Reply 
 
Udo Schlengermann
Consultant, -
Standards Consulting, Germany, Joined Nov 1998, 183

Udo Schlengermann

Consultant, -
Standards Consulting,
Germany,
Joined Nov 1998
183
04:48 Jan-15-2002
Re: Calibration Procedures for Immersion Ultrasound Testing
reply by Udo Schlengermann
:

If you look for general standards on ultrasonic immersion technique, please take a look at the following ASTM specifications:

ASTM E124 (2001)
Standard practice for immersed ultrasonic examination by the reflection-method using pulsed longitudinal waves.

ASTM E1001 (1999)
Standard practice for detection and evaluation of discontinuities by the immersed pulsed-echo ultrasonic method using longitudinal waves.

Reference
More details how to use the ultrasonic immersion technique for special test objects you can only get from handbooks or by special training courses.
Reference objects for calibration using immersion technique have to be made close to the original material, size and shape to be examined, containing artificial reflectors if necessary.
Kind regards
Udo Schlengermann
Agfa NDT GmbH

: Hi all,
.
: I am a researcher working on Ultrasound immersion testing of Aluminium parts.
: I have a copy of the Australian Standard 2083-1981 -- Calibration Blocks and their methods of use in Ultrasonic Testing,
: which explains basically about the ultrasound contact testing.
.
: My question is whether there are any separate calibration standards for ultrasound immersion testing.
: If so what are they.
.
: Thank you,
.
: Suresh Palanisamy
.



 
 Reply 
 
S.V.Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S.V.Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
08:47 Jan-20-2002
Re: Calibration Procedures for Immersion Ultrasound Testing
In immersion testing, the calibration standards have to be of the same size, shape, material and metalurgical condition, so that the time of travel in the calibration block and the actual test object remains same. As for the transit time for the signal in water, temperature compensation is needed and surface echo triggered gates are best so that the echoes from the test object follow the changes in the surface contour properly.

Swamy

: reply by Udo Schlengermann
: :
.
: If you look for general standards on ultrasonic immersion technique, please take a look at the following ASTM specifications:
.
: ASTM E124 (2001)
: Standard practice for immersed ultrasonic examination by the reflection-method using pulsed longitudinal waves.
.
: ASTM E1001 (1999)
: Standard practice for detection and evaluation of discontinuities by the immersed pulsed-echo ultrasonic method using longitudinal waves.
.
: Reference
: More details how to use the ultrasonic immersion technique for special test objects you can only get from handbooks or by special training courses.
: Reference objects for calibration using immersion technique have to be made close to the original material, size and shape to be examined, containing artificial reflectors if necessary.
: Kind regards
: Udo Schlengermann
: Agfa NDT GmbH
.
: : Hi all,
: .
: : I am a researcher working on Ultrasound immersion testing of Aluminium parts.
: : I have a copy of the Australian Standard 2083-1981 -- Calibration Blocks and their methods of use in Ultrasonic Testing,
: : which explains basically about the ultrasound contact testing.
: .
: : My question is whether there are any separate calibration standards for ultrasound immersion testing.
: : If so what are they.
: .
: : Thank you,
: .
: : Suresh Palanisamy
: .
.



 
 Reply 
 
amin
amin
11:47 Oct-24-2014
Re: Calibration Procedures for Immersion Ultrasound Testing
In Reply to Suresh Palanisamy at 00:05 Jan-15-2002 (Opening).

hi all,
i am final year student and working immersion testing of aluminium and steel.
my question what the standard dimension for plate and aluminium used in immersion testing and if yes,please attach with article and other information.

tq,
aminjunior

 
 Reply 
 
Hamid
Engineering, Researcher
Ecole de technologie superieure, Canada, Joined Sep 2012, 59

Hamid

Engineering, Researcher
Ecole de technologie superieure,
Canada,
Joined Sep 2012
59
23:48 Nov-07-2014
Re: Calibration Procedures for Immersion Ultrasound Testing
In Reply to Udo Schlengermann at 04:48 Jan-15-2002 .

Download Virus Scan recommended!

Hi,

I am trying to make reference block to measure the acoustic properties of a special class of steel. Actually, I am trying to use immersion testing method since I need the couplant layer to remain constant during the test. There will be some SDHs in the block. I am trying to avoid the interference between adjacent SDH reflection echos due to beam divergence; I would please like to know which of the images (in the attached document) is correct to be used for the design of the block.

Thanks

 
 Reply 
 

Product Spotlight

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

On Demand Webinar: Improve the Efficiency and Accuracy of Inspection Scanning

On-demand webinar on scanning technology that helps improve the efficiency and accuracy of ultrasoni
...
c inspections in oil and gas, aerospace, manufacturing and other industrial applications. The webinar features a scanning solution for multiple inspection environments, including flat and curved specimens, magnetic and nonmagnetic surfaces and raster scanning over long distances. View it today.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window