How common is it in europe or USA to Measure thickness of Steel Sheet pile in harbour´s and is it done by diver or R.O.V.?

I have been trying to find something about this on the internet and the resaults haven´t been so good.

I am asking because it has never been done here in Iceland.

Thank´s

Gisli


 
 Reply 
 
Simon Amallraja
Simon Amallraja
08:52 Feb-29-2008
Re: Underwater NDT
----------- Start Original Message -----------
: How common is it in europe or USA to Measure thickness of Steel Sheet pile in harbour´s and is it done by diver or R.O.V.?
: I have been trying to find something about this on the internet and the resaults haven´t been so good.
: I am asking because it has never been done here in Iceland.
: Thank´s
: Gisli
------------ End Original Message ------------

Force Technology of Denmark will help you. They have ROV type inspection for underwater applications.
www.forcetechnolgy.com

Simon


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
01:42 Feb-29-2008
Re: Underwater NDT
We have provided waterproof transducers and cables from the Panametrics-NDT product line for underwater inspection at depths greater than 50 meters. In most cases these applications have involved relatively shallow depths (tens of meters), with a diver manipulating the transducer while an observer on a dock or boat or oil platform monitors the instrument.


----------- Start Original Message -----------
: How common is it in europe or USA to Measure thickness of Steel Sheet pile in harbour´s and is it done by diver or R.O.V.?
: I have been trying to find something about this on the internet and the resaults haven´t been so good.
: I am asking because it has never been done here in Iceland.
: Thank´s
: Gisli
------------ End Original Message ------------




 
 Reply 
 
Peter Simpson
Director,
Ashtead Technology Ltd, United Kingdom, Joined Oct 1999, 12

Peter Simpson

Director,
Ashtead Technology Ltd,
United Kingdom,
Joined Oct 1999
12
03:48 Feb-29-2008
Re: Underwater NDT

There are two underwater ultrasonic thickness gauges available from Cygnus Instruments that can be used by ROV or Diver. Either system are available for rental from Ashtead Technology Ltd.


Best Regards


Peter

----------- Start Original Message -----------
: We have provided waterproof transducers and cables from the Panametrics-NDT product line for underwater inspection at depths greater than 50 meters. In most cases these applications have involved relatively shallow depths (tens of meters), with a diver manipulating the transducer while an observer on a dock or boat or oil platform monitors the instrument.
:
: : How common is it in europe or USA to Measure thickness of Steel Sheet pile in harbour´s and is it done by diver or R.O.V.?
: : I have been trying to find something about this on the internet and the resaults haven´t been so good.
: : I am asking because it has never been done here in Iceland.
: : Thank´s
: : Gisli
------------ End Original Message ------------




 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 528

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
528
00:41 Mar-01-2008
Re: Underwater NDT
If , as I would interpret the question, this is stanadrd interlocking steel piling then an ROV seems a bit excessive - Should be easy enough with a diver and a thickness gauge- Can be done either two-man with a long cable or using a submersible gauge - Our basic gauges (Sonagage III, Steelgage II or T-Gage IV, ) with a UMX enclosure would do the job, The Cygnus underwater gauges also seem to be well regarded.

Joe


----------- Start Original Message -----------
: How common is it in europe or USA to Measure thickness of Steel Sheet pile in harbour´s and is it done by diver or R.O.V.?
: I have been trying to find something about this on the internet and the resaults haven´t been so good.
: I am asking because it has never been done here in Iceland.
: Thank´s
: Gisli
------------ End Original Message ------------




 
 Reply 
 
Gisli A. Gudmundsson
Gisli A. Gudmundsson
02:06 Mar-03-2008
Re: Underwater NDT
Thanks guys for quick response.

Greetings from Iceland


 
 Reply 
 
Riccardo scottini
Riccardo scottini
00:47 Mar-12-2008
Re: Underwater NDT
Dear Gisli,

RTD-INCOTEST could be a solution for your purposes.

INCOTEST is a Pulsed Eddy Current equipment designed for corrosion detection and monitoring through insulation, therefore it does not need a direct contact with the object under examination.

We regularly use it to inspect and monitor Steel Sheet Piling conditions. It is efficient also in detecting Accelerated Low Water Corrosion in steel sheet piling, commonly used in harbours, Quay's, canals and dikes. ALWC can have a growth rate of 1 mm per year!

Operation normally with divers or Stick, sometime with ROV which are preferred when the inspection depth is more than 30m (example non piggable subsea pipelines in the North sea at approx. 140~160m depth), it does not need special surface cleaning and preparation, therefore it may detect corrosion trough coatings, concrete and marine growth.

For more information please contact me.
Regards,
Riccardo Scottini



 
 Reply 
 
andrea Bellizzi
Director,
Italy, Joined Feb 2015, 1

andrea Bellizzi

Director,
Italy,
Joined Feb 2015
1
14:54 Feb-24-2015
Re: Underwater NDT
In Reply to Riccardo scottini at 00:47 Mar-12-2008 .

Hi Riccardo,
may I have your contact mail or phone we are interesing in Pulse Eddy Current tecnology

 
 Reply 
 

Product Spotlight

VeeScan AirCraft Wheel Inspection

The VEESCAN offers maximum flexibility, has a proven mechanical design and records of breakdown-fr
...
ee operation of over 365 days. Appealing to companies in the Aerospace industry, the VEESCAN is ideal for all wheel-testing environments. With a wide selection of probes, the VeeScan allows your wheel testing facility the flexibility to select the most compatible configurations with their workload.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>