Crack detection

Dear All
We are producing punches and dies for the tabletting machines (presses) in the pharmaceutical industry. Currently, we have been sourcing a crack detection equipment (for very fine cracks) for surface and sub-surface cracks.Eventhough we have liquid penetrant and optical measurement equipment in place, these methods are time consuming eventhough very effective. The ideal method should detect the cracks within less than a minute. Our products are made of steel and average material thickness is 16 mm. If you suggest any method or equipment which allows us perform the test in less than a minute and also precise, this would be highly appreciated.
Meanwhile, we tried Eddy current method and this did not give the expectant results, was not effective. For more information about our products, you can visit our web site.
www.iholland.co.uk
Could Magnetic Particle-Fluorescent, Ultrasonic test or Magnetic Barkhausen Noise method be the answer?
Thank you in advance





 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 281

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
281
09:56 Jul-24-2003
Re: Crack detection
You might consider resistivity measurement. 4 point pin resisitivity measures very fine chganges in measurement resistance over a set pin spacing. Changes in resisitivity due to prescence of a crack are possible. Once set up properly it is less than a minute per spot. If you wish to pursue please contact me.


 
 Reply 
 
Jamie Gauthier
Jamie Gauthier
06:07 Jul-24-2003
Re: Crack detection
You might consider ACFM (Alternating Current Field Measurement). Very accurate and fast for measuring surface breaking cracks. Can work in high temperatures as well and gives a recordable image.


 
 Reply 
 
abdallah hassan
abdallah hassan
05:35 Aug-04-2003
Re: Crack detection
: You might consider resistivity measurement. 4 point pin resisitivity measures very fine chganges in measurement resistance over a set pin spacing. Changes in resisitivity due to prescence of a crack are possible. Once set up properly it is less than a minute per spot. If you wish to pursue please contact me.
.plz reply quickly either refuse or accept




 
 Reply 
 

Product Spotlight

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>