Inconnel625 2" 8.74mm best technique for meterial defects???

Gents,

Suggest a best technique to find materiel defect for 2inch 8.74mm inconnel625 meterial
To cover overall pipe from id to od, need to inspect entire length.

As of me IRIS is suitable
need other opinions in dis regards.

Thanks.

 
 Reply 
 
Johann Hinken
,
fitm Hinken Consult, Germany, Joined May 2014, 21

Johann Hinken

,
fitm Hinken Consult,
Germany,
Joined May 2014
21
15:05 Apr-08-2015
Re: Inconnel625 2" 8.74mm best technique for meterial defects???
In Reply to jagan at 14:18 Apr-04-2015 (Opening).

Hello,
in case you are interested in defects being ferromagnetic inclusions, I suggest magnetometry. That is a sensitive magnetic measurement after magnetisation. If you are interested I can give you more details.
Regards, Johann

 
 Reply 
 
R Dhanasekaran
Other, TEAM LEADER NDT
VESTAS WIND TECHNOLOGY INDIA PVT LTD, India, Joined Apr 2012, 15

R Dhanasekaran

Other, TEAM LEADER NDT
VESTAS WIND TECHNOLOGY INDIA PVT LTD,
India,
Joined Apr 2012
15
11:25 Apr-09-2015
Re: Inconnel625 2" 8.74mm best technique for meterial defects???
In Reply to jagan at 14:18 Apr-04-2015 (Opening).

Dear Jagan,

what kind of defects are you looking for?

i would not suggest IRIS for detecting Cracks.

Regards
R.Dhanasekaran

 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
12:13 Apr-09-2015
Re: Inconnel625 2" 8.74mm best technique for meterial defects???
In Reply to R Dhanasekaran at 11:25 Apr-09-2015 .

What length of pipe (tube) and how many pipes? Is that 8,74mm wall thickness?

I would recommend immersion UT with one probe sending sound in at 0 degrees looking for longitudinal defects and another compression wave offset from TDC to introduce shear wave looking for radial (through thickness) defects. Pipe (tube) will be rotated. There is a simple calculation based on ID/OD to determine optimum offset.

 
 Reply 
 
jagan
Engineering,
Saudi Arabia, Joined Dec 2011, 23

jagan

Engineering,
Saudi Arabia,
Joined Dec 2011
23
14:20 Apr-09-2015
Re: Inconnel625 2" 8.74mm best technique for meterial defects???
In Reply to Johann Hinken at 15:05 Apr-08-2015 .

Dear Johann Hinken,

Thanks forthe suggession.
can explain how it can be done
Magnetometry???

 
 Reply 
 
jagan
Engineering,
Saudi Arabia, Joined Dec 2011, 23

jagan

Engineering,
Saudi Arabia,
Joined Dec 2011
23
14:27 Apr-09-2015
Re: Inconnel625 2" 8.74mm best technique for meterial defects???
In Reply to Nigel Armstrong at 12:13 Apr-09-2015 .

Dear Nigel Armstrong,

Yse 8.74mm wall thickness 2inch dia and its 60 meter long spool with more than ten welds.
length is also an issue if we go for immersion.

thanks.

 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
14:42 Apr-09-2015
Re: Inconnel625 2" 8.74mm best technique for meterial defects???
In Reply to jagan at 14:27 Apr-09-2015 .

im amazed that you didnt consider giving this info origimally!

 
 Reply 
 
Johann Hinken
,
fitm Hinken Consult, Germany, Joined May 2014, 21

Johann Hinken

,
fitm Hinken Consult,
Germany,
Joined May 2014
21
16:30 Apr-09-2015
Re: Inconnel625 2" 8.74mm best technique for meterial defects???
In Reply to jagan at 14:20 Apr-09-2015 .

Hello Jagan,

the "magnetometry" consists of two steps: 1.) magnetizing the part in a strong dc magnetic field and 2.) scanning the surface of the part by a sensitive magnetometer which excludes the influence of background fields. The method is good for the detection of very small ferromagnetic inclusions in non-magnetic alloys like Inconel. We use it routinely in the inspection of aero engine turbine discs.

Regards, Johann

 
 Reply 
 

Product Spotlight

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window