Lining Thickness measurement

Dear Experts

Can the thickness of lining be measured in an internal cement lined pipe?

What other meathod is used to ensure uniform lining thickness in a smaller diameter piping having internal cement lining??

Thank you


 
 Reply 
 
Sasaki
Sasaki
08:28 Jul-22-2003
Re: Lining Thickness measurement
RT can be applicable to measure the thickness and the thickness uniformity of ganite lining of pipe inside.


 
 Reply 
 
Bijay Muduli
Engineering
IOCL, India, Joined Jul 2003, 4

Bijay Muduli

Engineering
IOCL,
India,
Joined Jul 2003
4
03:20 Aug-25-2003
Re: Lining Thickness measurement
I am inviting more opinions / (methods) on this subject.

Thanks & regards

B K Muduli


Dear Experts
.
: Can the thickness of lining be measured in an internal cement lined pipe?
.
: What other meathod is used to ensure uniform lining thickness in a smaller diameter piping having internal cement lining??
.
: Thank you
.



 
 Reply 
 
David Castle
David Castle
05:12 Apr-02-2005
Re: Lining Thickness measurement
: Dear Experts
.
: Can the thickness of lining be measured in an internal cement lined pipe?
.
: What other meathod is used to ensure uniform lining thickness in a smaller diameter piping having internal cement lining??
.
: Thank you
.

The thickness of cement lined pipe should be able to be measured using an eddy current device that is designed for the range of thicknesses that you are wanting to measure. I have used the Dinsearch DS500 for measuring Inconel cladding thickness in the range of 0 to 10 mm thickness with very good success. The company can be reached at:

Dinsley Devices Limited,
Ivy House, Streatlam Park,
County Durham, DL12 8TZ, UK.
Phone/Fax: +44 (0)1833 637971
email: dinsearch@hotmail.com

I hope that this is of help. Good Luck.
I hope that this may hekp you.



 
 Reply 
 
Charles Owston, Dinsley Devices Ltd
Charles Owston, Dinsley Devices Ltd
04:11 Apr-05-2005
Re: Lining Thickness measurement
----------- Start Original Message -----------
: : Dear Experts
: .
: : Can the thickness of lining be measured in an internal cement lined pipe?
: .
: : What other meathod is used to ensure uniform lining thickness in a smaller diameter piping having internal cement lining??
: .
: : Thank you
: .
: The thickness of cement lined pipe should be able to be measured using an eddy current device that is designed for the range of thicknesses that you are wanting to measure. I have used the Dinsearch DS500 for measuring Inconel cladding thickness in the range of 0 to 10 mm thickness with very good success. The company can be reached at:
: Dinsley Devices Limited,
: Ivy House, Streatlam Park,
: County Durham, DL12 8TZ, UK.
: Phone/Fax: +44 (0)1833 637971
: email: dinsearch@hotmail.com
: I hope that this is of help. Good Luck.
: I hope that this may hekp you.
------------ End Original Message ------------

At Dinsley Devices Ltd we have over 25 years of experience in providing inovative solutions to problems in the inspection of pipes.

If you care to send details of your problem we will see if we can offer a solution.



 
 Reply 
 

Product Spotlight

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

Echomac® PA Bar Tester

The Echomac® PA BT provides 100% inspection of round bars for core and surface defects, at speeds u
...
p to 2 m/sec, depending on the specific application. The unit allows producers to handle a much larger range of diameters in one installation, and is available in 3 models to test 10 – 75mm diameter (small model); 20 – 130mm (medium model) or 50 – 254mm (large model) bars.
>

VeeScan AirCraft Wheel Inspection

The VEESCAN offers maximum flexibility, has a proven mechanical design and records of breakdown-fr
...
ee operation of over 365 days. Appealing to companies in the Aerospace industry, the VEESCAN is ideal for all wheel-testing environments. With a wide selection of probes, the VeeScan allows your wheel testing facility the flexibility to select the most compatible configurations with their workload.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>