Aircraft weld incpection

I am a student at Faculty of Engineering and Naval Arhitecture in Zagreb. I am doing my final thesis and am looking for a Maintenance Manual or Component Repair and Overhaul Manual for any part of any type of any Boeing or Airbus aircraft, which defines inspection of welds (either steel or aluminum).
My intention is to simulate such a part in faculty`s labaratory (for I am unable to acquire a real-life part or documentation)and to perform prescribed radiografic (or ultrasonic) testing.
Materials can be on-line.


 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 526

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
526
06:50 Sep-08-2003
Re: Aircraft weld incpection
in my experience there are very few critical welded joints in Aircraft structures. Mostly just used in ancilliary assemblies, In particular in Ducting (e.g thin wall stainless or alloy tubes) and in landing gear.

----------- Start Original Message -----------
: I am a student at Faculty of Engineering and Naval Arhitecture in Zagreb. I am doing my final thesis and am looking for a Maintenance Manual or Component Repair and Overhaul Manual for any part of any type of any Boeing or Airbus aircraft, which defines inspection of welds (either steel or aluminum).
: My intention is to simulate such a part in faculty`s labaratory (for I am unable to acquire a real-life part or documentation)and to perform prescribed radiografic (or ultrasonic) testing.
: Materials can be on-line.
------------ End Original Message ------------




 
 Reply 
 
Gary
Consultant
TWI, United Kingdom, Joined May 2001, 15

Gary

Consultant
TWI,
United Kingdom,
Joined May 2001
15
02:31 Sep-11-2003
Re: Aircraft weld incpection
From my experience I have seen some fairly bad accidents through failures of welds in ductings, particularly with secondary damge to wiring looms etc.

Landing gear also has its uses on occassion.

----------- Start Original Message -----------
: in my experience there are very few critical welded joints in Aircraft structures. Mostly just used in ancilliary assemblies, In particular in Ducting (e.g thin wall stainless or alloy tubes) and in landing gear.
: : I am a student at Faculty of Engineering and Naval Arhitecture in Zagreb. I am doing my final thesis and am looking for a Maintenance Manual or Component Repair and Overhaul Manual for any part of any type of any Boeing or Airbus aircraft, which defines inspection of welds (either steel or aluminum).
: : My intention is to simulate such a part in faculty`s labaratory (for I am unable to acquire a real-life part or documentation)and to perform prescribed radiografic (or ultrasonic) testing.
: : Materials can be on-line.
------------ End Original Message ------------




 
 Reply 
 
Carlos Valdecantos
Engineering
MTORRES, Ing., Spain, Joined May 2001, 9

Carlos Valdecantos

Engineering
MTORRES, Ing.,
Spain,
Joined May 2001
9
01:07 Sep-12-2003
Re: Aircraft weld incpection
AIRBUS is currently using welded stringers as an alternative to massive machinning of thick plates. Welding is carried out by high power laser.

Our company is the supplier of the automatic machines for this process. Please, refer to MTORRES web site.

Regards,

C. Valdecantos



 
 Reply 
 

Product Spotlight

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

Navic - Steerable Modular Automated Scanner

The Navic is a modular, motorized, steerable scanner designed to carry multiple attachments used
...
in various scanning and inspection applications. The Navic is capable of weld scanning (girth welds and long seam welds), automated corrosion mapping, and tank scanning.
>

MIZ®-21C: Truly Affordable Eddy Current Handheld with Surface Array Capability

Introducing MIZ-21C, the first truly affordable handheld eddy current instrument with surface array
...
capabilities. MIZ-21C can deliver fast, accurate inspections in demanding NDT applications including aerospace, oil and gas, manufacturing, and power generation. The surface array solution can reduce inspection time by up to 95% compared to traditional handheld pencil probes. The ergonomic design, long battery life, and intuitive touchscreen mean you can inspect more areas faster than ever without fatigue.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window