where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

Hillger NDT GmbH
was founded in 1984 and develops special ultrasonic imaging systems for high-tech materials.
491 views
Technical Discussions
Bijay Muduli
Engineering
IOCL, India, Joined Jul 2003, 4

Bijay Muduli

Engineering
IOCL,
India,
Joined Jul 2003
4
08:40 Oct-10-2003
Ultrasonics for Cement Lining

1) Is there any Ultrasonic technique to measure lining/ coating thickness on steel pipes?

2) Can dual probes help in this regard?

Your valuable replies shall be appreciated.

Regards



 
 Reply 
 
Todd Allen
Consultant, Ground Penetrating Radar ( GPR )
Radarview Concrete and Underground 3D Imaging, USA, Joined Jan 2003, 7

Todd Allen

Consultant, Ground Penetrating Radar ( GPR )
Radarview Concrete and Underground 3D Imaging,
USA,
Joined Jan 2003
7
01:41 Oct-13-2003
Re: Ultrasonics for Cement Lining
----------- Start Original Message -----------
: 1) Is there any Ultrasonic technique to measure lining/ coating thickness on steel pipes?
: 2) Can dual probes help in this regard?
: Your valuable replies shall be appreciated.
: Regards
------------ End Original Message ------------

Hello,

Yes, there are a few methods that could be used to measure the thickness of concrete / cement linings and or coatings. The 1st is Ground Penetrating Radar which will measure the thickness of the concrete by detecting the strong dielectric change at the concrete-steel interface. This method must be done from the concrete side not the steel side.
The 2nd method is Impact Echo testing which essentially uses very low frequency impacts on the concrete surface. The frequency response from the echo at the interface can be correlated to a thickness.
The 3rd method would be to use Radiography to get a profile image of the pipe. This method may/may not work depending on the size and thickness of the pipe and concrete.

Thanks,
Todd Allen
Radarview Structural and Underground Services
281-705-9476


 
 Reply 
 
Bijay Muduli
Engineering
IOCL, India, Joined Jul 2003, 4

Bijay Muduli

Engineering
IOCL,
India,
Joined Jul 2003
4
02:08 Oct-16-2003
Re: Ultrasonics for Cement Lining
----------- Start Original Message -----------
: : 1) Is there any Ultrasonic technique to measure lining/ coating thickness on steel pipes?
: : 2) Can dual probes help in this regard?
: : Your valuable replies shall be appreciated.
: : Regards
: Hello,
: Yes, there are a few methods that could be used to measure the thickness of concrete / cement linings and or coatings. The 1st is Ground Penetrating Radar which will measure the thickness of the concrete by detecting the strong dielectric change at the concrete-steel interface. This method must be done from the concrete side not the steel side.
: The 2nd method is Impact Echo testing which essentially uses very low frequency impacts on the concrete surface. The frequency response from the echo at the interface can be correlated to a thickness.
: The 3rd method would be to use Radiography to get a profile image of the pipe. This method may/may not work depending on the size and thickness of the pipe and concrete.
: Thanks,
: Todd Allen
: Radarview Structural and Underground Services
: 281-705-9476
------------ End Original Message ------------

Thank you verymuch Mr Allen.




 
 Reply 
 

Product Spotlight

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

YXLON Cougar EVO

Scalable small footprint X-ray inspection systems for assembly and laboratory applications. The
...
YXLON Cougar EVO series was designed to provide the "best-in- class" inspection solutions for SMT, semiconductor, and laboratory assembly applications, while maintaining a small system footprint for maximum convenience. With optimized software and hardware, these systems produce higher quality and more consistent results than other electronics inspection systems currently on the market.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>