MPT of Stainless steel

Why Magnetic particle testing is not possible for Stainless steel?

1
 
 Reply 
 
anjafo79
NDT Inspector
Norway, Joined Aug 2009, 204

anjafo79

NDT Inspector
Norway,
Joined Aug 2009
204
12:33 Sep-28-2009
Re: MPT of Stainless steel
In Reply to ravi prajapati at 11:22 Sep-28-2009 (Opening).

most simply put it is not magnetic enough.

1
 
 Reply 
 
Chris Galay
NDT Inspector
Portugal, Joined Sep 2009, 2

Chris Galay

NDT Inspector
Portugal,
Joined Sep 2009
2
23:48 Sep-28-2009
Re: MPT of Stainless steel
In Reply to ravi prajapati at 11:22 Sep-28-2009 (Opening).

The reason why stainless steel cannot be inspected by magnetic particle testing is that we cannot induce a magnetic field on the material as this is non-magnetic. We need a flux leakage so a magnetic field must be present. I hope this will help in your query.

Chris

1
 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
03:10 Sep-29-2009
Re: MPT of Stainless steel
In Reply to anjafo79 at 12:33 Sep-28-2009 .

Its only the austenitic stainless steels which are incapable of magnetisation. The ferritic stainless steels ARE ferromagnetic. Apply a small permanent magnet to the test-piece if you are uncertain whether a material is austenitic or ferritic stainless steel.

2
 
 Reply 
 
Tom Colter
Engineering,
Bechtel Plant Machinery Inc., USA, Joined Nov 1998, 3

Tom Colter

Engineering,
Bechtel Plant Machinery Inc.,
USA,
Joined Nov 1998
3
00:55 Sep-30-2009
Re: MPT of Stainless steel
In Reply to ravi prajapati at 11:22 Sep-28-2009 (Opening).

For a good expalanation of which stainless steels are paramagnetic (can't be subjected to MPT) and which ones are ferromagnetic (can be subjected to MPT) go to this link:
Magnetic Stainless Steel or Not

1
 
 Reply 
 
Jim Draper
Consultant, ASNT Level III MT PT RT VT
Draper NDT, USA, Joined Jul 2009, 99

Jim Draper

Consultant, ASNT Level III MT PT RT VT
Draper NDT,
USA,
Joined Jul 2009
99
01:17 Sep-30-2009
Re: MPT of Stainless steel
In Reply to Tom Colter at 00:55 Sep-30-2009 .

It is true that you can perform mag particle testing on ferritic stainless steels. The easiest method of determining if the material can be mag particle inspected is to see if a permanent magnet is attracted to it. The three elements which are ferromagnetic are iron, nickel and cobalt.

1
 
 Reply 
 
NIMBANNA
NIMBANNA
07:11 Oct-01-2015
Re: MPT of Stainless steel
In Reply to ravi prajapati at 11:22 Sep-28-2009 (Opening).

All stainless steel materials are nonferrous hence not possible for magnetise the same. For magnetic particle testing, flux leakage is must which is not possible in this case. Hence Magnetic particle testing is not possible. To find out the defects, we may carry out RT / UT which will suffice the requirements.

1
 
 Reply 
 
S V Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S V Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
09:26 Oct-01-2015
Re: MPT of Stainless steel
In Reply to NIMBANNA at 07:11 Oct-01-2015 .

Pl. correct your understanding of the subject of stainless steels. All stainless steels are not non-magnetic - ferritic stainless steels and martensitic stainless steels etc. are magnetic. Only austenitic stainless steels in fully annealed condition are non-magnetic (paramagnetic).

Best regards

S V Swamy
Metallurgist and Quality / NDT professional (now retired)

3
 
 Reply 
 
Narayana Prasad.N
Narayana Prasad.N
13:00 Oct-01-2015
Re: MPT of Stainless steel
In Reply to NIMBANNA at 07:11 Oct-01-2015 .

I disagree with your statement that all stainless steels are non ferrous
Regards

3
 
 Reply 
 
Hello Sir
Engineering, welding inspector
Tekfen, India, Joined Sep 2009, 1

Hello Sir

Engineering, welding inspector
Tekfen,
India,
Joined Sep 2009
1
06:47 Feb-20-2017
Re: MPT of Stainless steel
In Reply to Jim Draper at 01:17 Sep-30-2009 .

Hi

Is it possible to perform MPI on Feritic Austenitic steel? pls explain sir

 
 Reply 
 
S V Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S V Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
08:42 Feb-20-2017
Re: MPT of Stainless steel
In Reply to Hello Sir at 06:47 Feb-20-2017 .

Ferritic Austenitic Stainless Steels also called duplex steel could be magnetic. As already explained earlier, check whether the material is magnetic or not using a permanent magnet. If the magnet is attracted to the material, MPT is feasible.

Swamy

 
 Reply 
 

Product Spotlight

VeeScan AirCraft Wheel Inspection

The VEESCAN offers maximum flexibility, has a proven mechanical design and records of breakdown-fr
...
ee operation of over 365 days. Appealing to companies in the Aerospace industry, the VEESCAN is ideal for all wheel-testing environments. With a wide selection of probes, the VeeScan allows your wheel testing facility the flexibility to select the most compatible configurations with their workload.
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window