ravi prajapati
ravi prajapati
11:22 Sep-28-2009
MPT of Stainless steel

Why Magnetic particle testing is not possible for Stainless steel?

1
 
 Reply 
 
anjafo79
NDT Inspector
Norway, Joined Aug 2009, 204

anjafo79

NDT Inspector
Norway,
Joined Aug 2009
204
12:33 Sep-28-2009
Re: MPT of Stainless steel
In Reply to ravi prajapati at 11:22 Sep-28-2009 (Opening).

most simply put it is not magnetic enough.

1
 
 Reply 
 
Chris Galay
NDT Inspector
Portugal, Joined Sep 2009, 2

Chris Galay

NDT Inspector
Portugal,
Joined Sep 2009
2
23:48 Sep-28-2009
Re: MPT of Stainless steel
In Reply to ravi prajapati at 11:22 Sep-28-2009 (Opening).

The reason why stainless steel cannot be inspected by magnetic particle testing is that we cannot induce a magnetic field on the material as this is non-magnetic. We need a flux leakage so a magnetic field must be present. I hope this will help in your query.

Chris

1
 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
03:10 Sep-29-2009
Re: MPT of Stainless steel
In Reply to anjafo79 at 12:33 Sep-28-2009 .

Its only the austenitic stainless steels which are incapable of magnetisation. The ferritic stainless steels ARE ferromagnetic. Apply a small permanent magnet to the test-piece if you are uncertain whether a material is austenitic or ferritic stainless steel.

2
 
 Reply 
 
Tom Colter
Engineering,
Bechtel Plant Machinery Inc., USA, Joined Nov 1998, 3

Tom Colter

Engineering,
Bechtel Plant Machinery Inc.,
USA,
Joined Nov 1998
3
00:55 Sep-30-2009
Re: MPT of Stainless steel
In Reply to ravi prajapati at 11:22 Sep-28-2009 (Opening).

For a good expalanation of which stainless steels are paramagnetic (can't be subjected to MPT) and which ones are ferromagnetic (can be subjected to MPT) go to this link:
Magnetic Stainless Steel or Not

1
 
 Reply 
 
Jim Draper
Consultant, ASNT Level III MT PT RT VT
Draper NDT, USA, Joined Jul 2009, 99

Jim Draper

Consultant, ASNT Level III MT PT RT VT
Draper NDT,
USA,
Joined Jul 2009
99
01:17 Sep-30-2009
Re: MPT of Stainless steel
In Reply to Tom Colter at 00:55 Sep-30-2009 .

It is true that you can perform mag particle testing on ferritic stainless steels. The easiest method of determining if the material can be mag particle inspected is to see if a permanent magnet is attracted to it. The three elements which are ferromagnetic are iron, nickel and cobalt.

1
 
 Reply 
 
NIMBANNA
NIMBANNA
07:11 Oct-01-2015
Re: MPT of Stainless steel
In Reply to ravi prajapati at 11:22 Sep-28-2009 (Opening).

All stainless steel materials are nonferrous hence not possible for magnetise the same. For magnetic particle testing, flux leakage is must which is not possible in this case. Hence Magnetic particle testing is not possible. To find out the defects, we may carry out RT / UT which will suffice the requirements.

1
 
 Reply 
 
S V Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S V Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
09:26 Oct-01-2015
Re: MPT of Stainless steel
In Reply to NIMBANNA at 07:11 Oct-01-2015 .

Pl. correct your understanding of the subject of stainless steels. All stainless steels are not non-magnetic - ferritic stainless steels and martensitic stainless steels etc. are magnetic. Only austenitic stainless steels in fully annealed condition are non-magnetic (paramagnetic).

Best regards

S V Swamy
Metallurgist and Quality / NDT professional (now retired)

3
 
 Reply 
 
Narayana Prasad.N
Narayana Prasad.N
13:00 Oct-01-2015
Re: MPT of Stainless steel
In Reply to NIMBANNA at 07:11 Oct-01-2015 .

I disagree with your statement that all stainless steels are non ferrous
Regards

3
 
 Reply 
 
Hello Sir
Engineering, welding inspector
Tekfen, India, Joined Sep 2009, 1

Hello Sir

Engineering, welding inspector
Tekfen,
India,
Joined Sep 2009
1
06:47 Feb-20-2017
Re: MPT of Stainless steel
In Reply to Jim Draper at 01:17 Sep-30-2009 .

Hi

Is it possible to perform MPI on Feritic Austenitic steel? pls explain sir

 
 Reply 
 
S V Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S V Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
08:42 Feb-20-2017
Re: MPT of Stainless steel
In Reply to Hello Sir at 06:47 Feb-20-2017 .

Ferritic Austenitic Stainless Steels also called duplex steel could be magnetic. As already explained earlier, check whether the material is magnetic or not using a permanent magnet. If the magnet is attracted to the material, MPT is feasible.

Swamy

 
 Reply 
 

Product Spotlight

GUL Subsea Solutions - Screeening & Monitoring

To inspect new and existing subsea lines, you need proven technology and experience. GUL offers it's
...
technology to solve this challenge: GUL Subsea and gMAT Transducer Rings.
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window