07:21 Feb-02-1999
UT on Inconel Weld Overlays

You should try to work with special Phased Array probes. We have developped such probes with a separated Transmitter Receiver operation for Longitudinal waves.
The probe has a size of about 25 x 25 mm, works at 3 MHz and allows as well the focussing at variable depth as the variation of the incidence angles between 36° and 76°.
More details can be received from the indicated E-mail address or from Mr. Guenter Engl at Siemens Erlangen (guenter.engl@erl11.siemens.de)

Hermann Wuestenberg


 
 Reply 
 

Product Spotlight

Micro CT

nanoVoxel series has nano-scale resolution by using high voltage X-ray source (from 80-300 kV) wit
...
h micro focal spot and highly sensitive detector including different kinds of big size panel detectors and lens coupling CCD.
>

GUL Subsea Solutions - Screeening & Monitoring

To inspect new and existing subsea lines, you need proven technology and experience. GUL offers it's
...
technology to solve this challenge: GUL Subsea and gMAT Transducer Rings.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window