Hello,

I'm a futur engineer.
For a study I'm looking for sofwares which could simulate the propagation of ultrasonics waves into a simple structure (plates or pipes) made with an elastic or viscoelastic material.
The structure has to be coupled with fluids.

At first sight, I thought at Femlab, Wave2000 or Disperse. Am I true ?
Where should I found more informations on the way they simulate the fluid-solid coupling ?

Do you know other sofwares that could simulate that case ?

Thanks a lot for any information you could give me.
Best regards


 
 Reply 
 
Richard D Finlayson
Director, Operations
Princeton Instruments, USA, Joined Jun 2000, 8

Richard D Finlayson

Director, Operations
Princeton Instruments,
USA,
Joined Jun 2000
8
09:47 Dec-04-2003
Re: Search ultrasonic modelling software for NDT
Vincent,

Our company (Physical Acoustics Corp.), has developed software that allows you to calculate Phase and Group velocity dispersion curves for elastic plates with different fluids on both sides. If this is the type of software that you are looking for, please contact me and I will discuss this further with you.

Richard


----------- Start Original Message -----------
: Hello,
: I'm a futur engineer.
: For a study I'm looking for sofwares which could simulate the propagation of ultrasonics waves into a simple structure (plates or pipes) made with an elastic or viscoelastic material.
: The structure has to be coupled with fluids.
: At first sight, I thought at Femlab, Wave2000 or Disperse. Am I true ?
: Where should I found more informations on the way they simulate the fluid-solid coupling ?
: Do you know other sofwares that could simulate that case ?
: Thanks a lot for any information you could give me.
: Best regards
------------ End Original Message ------------




 
 Reply 
 
Wolfgang Bisle
R & D, senior Engineer and nomiated Expert
retired from Airbus Deutschland GmbH, Germany, Joined Jul 2000, 37

Wolfgang Bisle

R & D, senior Engineer and nomiated Expert
retired from Airbus Deutschland GmbH,
Germany,
Joined Jul 2000
37
06:16 Jan-05-2004
Re: Search ultrasonic modelling software for NDT
Raelly an interesting subject.

We are also on the search for a good solution.
But it should be a commercial one.
Not an academic, but a commercial available one.
And a code which can be used by a simple level II inspector and not by a specialist for numerical mathematics.

There are nice codes available at universities - here for instance AFIT & EFIT (Ultrasound) from the GH Kassel, Prof. Langenberg or MAFIA (Electrical Fields, Eddy Current...) from TU Darmstadt. But where is a commercial software distributor available, who cares for the needs of the customer.

So finally the remaining product is somewhat like CIVA, a "something" assembled from lot's of different sources, with a lousy user interface, full of bugs,
lots of program crashes, if you miss the right button, but in general the only code which covers a little more than just primitive raytracing of single element transducers.

Where is the commercial available code to modell beam characteristics of Array transducers?
Where is a code to modell anisotropic materials, which can be used by a simple levle II inspector?
where is a code, where you can interface your CAD program and your inspection system to transfer the focal laws - with a customer support?

We checked the market and found nothing better then CIVA by CEA.

Or do you have a better idea? Finally I found out, that some other big players in NDT went the same way. Checked the market and found: Noone except CIVA to be good enough to really support the product and the customer.
Please note: it is not enough just to sell something.
We need a worldwide support with a hotline to place questions if we can't solve our virtual inspection problem.
With the current situation we are completely not satisfied. But hearing around, we found there are some groups in the world working on NDT Modelling. But nearly nobody is able to bring a satisfying product on the market, which can be really used by a non-specialist of numerical mathematics.
I would be happy if you can show methe opposite. But come to me. Don't ask me to come to you. Then you are not able to do support. And nothing is more important to be able to support the product.


 
 Reply 
 

Product Spotlight

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Echomac® PA Tube Weld Tester

The new robotic Echomac® PA TW is an operator friendly test system for detecting weld zone defects
...
in tube and pipe caused by scarfing or welding processes. Electronic scanning ensures that the entire weld zone is covered without the need for mechanical movement or operator adjustment.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Extended Range Variable Wall® Piping Calibration Blocks for Longseam Inspection

This set of two blocks has been specially designed for situations where ultrasonic examination tak
...
es place circumferentially or “around the curve” for applications such as inspection of longseam welds in piping and vessels. Jointly designed by PH Tool and Holloway NDT, the blocks feature side-drilled hole reflectors positioned within novel compound-curves, each with multiple thickness steps. The unique design results in a light and compact form factor, with the largest block weighing just over 15 lbs and spanning just 16 ¾”. Coverage is provided for nominal pipe sizes from 6” to 10” in the small block and 12” to a whopping 56” in the large block. The compound OD curves and multiple wall thicknesses actually exceed ASME requirements, providing exceptional signal response and measurement accuracy. Properly managing beam divergence off the ID and stabilizing beam skew due to probe rocking is essential to maintaining a consistent calibration when inspecting lengthwise on curved surfaces.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window