Acoustic Absorption Coefficients

Hi. Does anyone know of a good book on 'properties of material' that also contains information such as the acoustic absorption coeffiecinet for those materials. Specifically I would like to attain the absorption coefficients for polystyrene, polypropylene, and polyethylene.

-hector


 
 Reply 
 
Wies³aw Bicz
Wies³aw Bicz
01:14 Feb-10-1999
Re: Acoustic Absorption Coefficients
: Hi. Does anyone know of a good book on 'properties of material' that also contains information such as the acoustic absorption coeffiecinet for those materials. Specifically I would like to attain the absorption coefficients for polystyrene, polypropylene, and polyethylene.

: -hector

You can find this information in many books, but it wont help you very much. There are many kinds of plastics on the market, having
different properties. Absorbtion is also very frequency dependent. It is much better to measure it. If you don´t need very high accuracy it is not difficult.
If you need a high accuracy we can help you - we are working on a device doing all such measurements with high accuracy.

W. Bicz


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
05:13 Feb-10-1999
Re: Acoustic Absorption Coefficients



 
 Reply 
 
Grant Gordon
Grant Gordon
06:49 Feb-10-1999
Re: Acoustic Absorption Coefficients
Greetings Hector,
I have recently measured the frequency dependent attenuation values for polycarbonate, acrylic,
linear low density polyethylene, PVC, and a polybutadiene over the frequency range of 1.5 - 9 MHz.
These results are part of a paper to be published in the SPIE Conference proceedings
on Ultrasonic Transducer Engineering to be held in San Diego CA, 20-26 February, 1999. If you are
interested I will send you a hard copy via mail - the electronic file is quite large.
Sincerley
Grant Gordon





 
 Reply 
 
Robert A. Day
Engineering
Milky Way Jewels, USA, Joined Nov 1998, 40

Robert A. Day

Engineering
Milky Way Jewels,
USA,
Joined Nov 1998
40
02:16 Feb-10-1999
Re: Acoustic Absorption Coefficients
: Hi. Does anyone know of a good book on 'properties of material' that also contains information such as the acoustic absorption coeffiecinet for those materials. Specifically I would like to attain the absorption coefficients for polystyrene, polypropylene, and polyethylene.

: -hector

I would also recommend Alan Selfridge's paper on measuring ultrasonic properties. His procedure is one of the best procedures for quick reasonably accurate measurements.

I would also warn you that polymers often have different acoustic properties depending on the conditions of manufacture. This includes thicknes as well as temperature and the actual chemistry used. It is essential to keep this in mind when making samples to measure. Thin layers are frequently different than the bulk.


 
 Reply 
 
gina
gina
06:13 Apr-01-2000
Re: Acoustic Absorption Coefficients
: Hi. Does anyone know of a site that will give me a list of materials and their absorption coefficients?

gina


 
 Reply 
 
yuksel guney
yuksel guney
01:42 May-08-2000
Re: Acoustic Absorption Coefficients of polyvinyldenefloride
: : Hi. Does anyone know of a good book on 'properties of material' that also contains information such as the acoustic absorption coeffiecinet for those materials. Specifically I would like to attain the absorption coefficients for polystyrene, polypropylene, and polyethylene.

: : -hector

: You can find this information in many books, but it wont help you very much. There are many kinds of plastics on the market, having
: different properties. Absorbtion is also very frequency dependent. It is much better to measure it. If you don´t need very high accuracy it is not difficult.
: If you need a high accuracy we can help you - we are working on a device doing all such measurements with high accuracy.

: W. Bicz




 
 Reply 
 
paco
paco
07:57 Oct-13-2000
Re: Acoustic Absorption Coefficients
: : Hi. Does anyone know of a good book on 'properties of material' that also contains information such as the acoustic absorption coeffiecinet for materials.


 
 Reply 
 
Ales Globevnik
Ales Globevnik
02:27 Mar-22-2002
Re: Acoustic Absorption Coefficients
Hellooo , I am also looking for absorption coefficients for materials. Please let me know if anybody know where can I found them.



 
 Reply 
 

Product Spotlight

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window