Hi

Sometimes we find LPG cylinders leaking around the circumferential weld during first filling at LPG bottling plants. Cylinders then sent to labs for failure analaysis. They carry out the leakage test with water and Pneumatic pressure. Most of the times, they could not establish any leakage from the same cylinders.

Why it happens and is their any better method, by which we can establish the leakage.



 
 Reply 
 
N.Kuppusamy
Consultant, NDT Level-III Engineer
Advanced Inspection & Testing (S) Pte Ltd, Singapore, Joined Dec 2003, 34

N.Kuppusamy

Consultant, NDT Level-III Engineer
Advanced Inspection & Testing (S) Pte Ltd,
Singapore,
Joined Dec 2003
34
00:25 Jan-02-2004
Re: Leakage of LPG cylinders
Hello,

Happy New Year to every body. You can advise your lab to perform hologen leak testing or Mass Spectrometer Test. These leak testings are more sensitive than others.

Regards,
N.Kuppusamy

----------- Start Original Message -----------
: Hi
: Sometimes we find LPG cylinders leaking around the circumferential weld during first filling at LPG bottling plants. Cylinders then sent to labs for failure analaysis. They carry out the leakage test with water and Pneumatic pressure. Most of the times, they could not establish any leakage from the same cylinders.
: Why it happens and is their any better method, by which we can establish the leakage.
------------ End Original Message ------------




 
 Reply 
 
Mike
NDT Inspector
Materiaal Metingen Holland, Netherlands, Joined Oct 1999, 2

Mike

NDT Inspector
Materiaal Metingen Holland,
Netherlands,
Joined Oct 1999
2
04:59 Jan-03-2004
Re: Leakage of LPG cylinders
----------- Start Original Message -----------
: Hi
: Sometimes we find LPG cylinders leaking around the circumferential weld during first filling at LPG bottling plants. Cylinders then sent to labs for failure analaysis. They carry out the leakage test with water and Pneumatic pressure. Most of the times, they could not establish any leakage from the same cylinders.
: Why it happens and is their any better method, by which we can establish the leakage.
------------ End Original Message ------------


You could try a dye penetrant test on the weld and surrounding area. This would probably be the cheapest option and quite easy. Any paint would have to be removed first.



 
 Reply 
 
Suleyman Halicioglu
Suleyman Halicioglu
08:00 Jan-05-2004
Re: Leakage of LPG cylinders
----------- Start Original Message -----------
: : Hi
: : Sometimes we find LPG cylinders leaking around the circumferential weld during first filling at LPG bottling plants. Cylinders then sent to labs for failure analaysis. They carry out the leakage test with water and Pneumatic pressure. Most of the times, they could not establish any leakage from the same cylinders.
: : Why it happens and is their any better method, by which we can establish the leakage.
:
: You could try a dye penetrant test on the weld and surrounding area. This would probably be the cheapest option and quite easy. Any paint would have to be removed first.
------------ End Original Message ------------

You should clean the weld and HAZ by brush or similar method and try a magnetic particle test, by yoke or prod type. You should perform the pneumatic test under water.


 
 Reply 
 
ALBERTO MONICI
Engineering, Leak Detection Service - Thermography Service -
ETS Sistemi Industriali, Italy, Joined Aug 2002, 17

ALBERTO MONICI

Engineering, Leak Detection Service - Thermography Service -
ETS Sistemi Industriali,
Italy,
Joined Aug 2002
17
00:06 Jan-05-2004
Re: Leakage of LPG cylinders
Hi, and Happy New Year to everybody!
The Pneumatic and Water Leak Test are able to find gross leak (more than 1*10-3 std cc/sec, in normal industrial labs application). For Leak below this value, you can find a pressure decreases but it is very difficult to localize the leak.
Also I suggest you to use Leak Detector in sniffer mode. I suggest to utilise Helium Leak Detector because Helium is a Noble Gas. More normatives (ASNT or EN) permit you to certify also the quantity of leaks with personnel qualified II level or more.
Our company furnish consultancy, automatic systems and services for Leak Test.
Alberto Monici
ETS Sistemi Industriali
Italy
----------- Start Original Message -----------
: Hello,
: Happy New Year to every body. You can advise your lab to perform hologen leak testing or Mass Spectrometer Test. These leak testings are more sensitive than others.
: Regards,
: N.Kuppusamy
:
: : Hi
: : Sometimes we find LPG cylinders leaking around the circumferential weld during first filling at LPG bottling plants. Cylinders then sent to labs for failure analaysis. They carry out the leakage test with water and Pneumatic pressure. Most of the times, they could not establish any leakage from the same cylinders.
: : Why it happens and is their any better method, by which we can establish the leakage.
------------ End Original Message ------------





 
 Reply 
 
HaccpMTC grp
HaccpMTC grp
08:00 Aug-09-2004
Re: Leakage of LPG cylinders
hi to every body

we are looking for the test system used to test the lpg cylinders e.g hydrostatic test system,ultrasonic test system ,corrossion test system and the valve test system.
looking for cooperation

Atif A.G.othman
g.director



 
 Reply 
 

Product Spotlight

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>