Magnetic particle testing


Hi,

My question is if we can detect the near-surface defects by magnetizing by yokes, if it is possible, what is the maximum thikness that we can controle.
The difference between the yoke magnetizing technic and the universal bunchs


 
 Reply 
 
Bruce Owen
Sales, Manufacturing
Lectromax Australia Pty Ltd, Australia, Joined Aug 2001, 2

Bruce Owen

Sales, Manufacturing
Lectromax Australia Pty Ltd,
Australia,
Joined Aug 2001
2
02:46 Jan-07-2004
Re: Magnetic particle testing
Hi Kais,
Before i attempt to give you an answer, what exactly do you mean "what is the maximum thickness that we can control" also, "the universal bunchs".
regards, Bruce.


 
 Reply 
 
BOUAZIZ KAIS
BOUAZIZ KAIS
09:15 Jan-08-2004
Re:Re: Magnetic particle testing
----------- Start Original Message -----------
: Hi Kais,
: Before i attempt to give you an answer, what exactly do you mean "what is the maximum thickness that we can control" also, "the universal bunchs".
: regards, Bruce.
------------ End Original Message ------------


"the maximum thickness" is the mesurement of the penetration of the magnetic fields in the part that we test,and "Universal bunchs" is the "direct contact magnetization through Head/Tailstock".
Best regards
Kais BOUAZIZ.



 
 Reply 
 
swapnil anjikar
swapnil anjikar
02:38 Sep-01-2004
Re: want a problem on Magnetic particle testing
respected sir
i am the student , studing in master degree in advanced manufacturing process , i am intrested in magnetic partical ins. tech . i done lots of litrature survy in this tech, i want a project in this tech. for my fullfillment of master degree . so pls help me , pls suggest me the problem in this tech. so i concentrate on that . took as my project
yous faithfully
swapnil d anjikar


 
 Reply 
 

Product Spotlight

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window