where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

Ultrasonic Sciences Ltd
We specialize in the design and manufacture of automated and semi-automated ultrasonic testing systems, including multi axis, multi channels systems and phased array electronics.
1015 views
Technical Discussions
vengadesh
Engineering,
Tech Mahindra LTD, India, Joined Mar 2016, 4

vengadesh

Engineering,
Tech Mahindra LTD,
India,
Joined Mar 2016
4
13:03 Mar-29-2016
probe output

Dear sir,
I have one doubt ,please help. we have 60 degree probe the prespex shoe was thickness reduced, due to continuous friction . the output of probe wavelength was changed into 65 degree. how can i draw DAC.? for that what is the formula for that..?

 
 Reply 
 
joan pagnoul
Student,
Technifutur, Belgium, Joined Mar 2014, 7

joan pagnoul

Student,
Technifutur,
Belgium,
Joined Mar 2014
7
15:19 Mar-29-2016
Re: probe output
In Reply to vengadesh at 13:03 Mar-29-2016 (Opening).

I think that first, your probe is useless because if I remember norms says 60+/-2 degrees.
And to draw a DAC, methods never change and there is no formula

1
 
 Reply 
 
Csaba Hollo
,
Retired, Canada, Joined Feb 2010, 301

Csaba Hollo

,
Retired,
Canada,
Joined Feb 2010
301
23:29 Mar-29-2016
Re: probe output
In Reply to vengadesh at 13:03 Mar-29-2016 (Opening).

If the code allows you to work with an angle outside of the 60 degree+-, then your calibrations, including regenerating your DAC, must be redone.
Several things have changed, not just your angle, but also your index point and most likely sensitivity.

1
 
 Reply 
 
massimo carminati
Consultant, AUT specialist
IMG Ultrasuoni Srl, Italy, Joined Apr 2007, 691

massimo carminati

Consultant, AUT specialist
IMG Ultrasuoni Srl,
Italy,
Joined Apr 2007
691
19:37 Mar-30-2016
Re: probe output
In Reply to vengadesh at 13:03 Mar-29-2016 (Opening).

Most codes would not allow you to use such a drifted angle from standard. You should recondition the probe or the wedge by adding a new wear sole, but before that you should bring back the original wedge angle to the original value. I warmly not suggest to just use sand paper for doing this.

 
 Reply 
 

Product Spotlight

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>