Technical Discussions
Zaheer
NDT Inspector, and as trainer
NDT Centre Pakistan, Pakistan, Joined Aug 2003, 2

Zaheer

NDT Inspector, and as trainer
NDT Centre Pakistan,
Pakistan,
Joined Aug 2003
2
00:06 Aug-14-2003
ASME Standard for spot Radiography


Dear Sir,
Last week we were discussing in a training course, the acceptance criteria of radiographic testing given in ASME 2001, section VIII Division 1 UW-52 for spot radiography.
Our interpretation of Para UW-52 (c) (2) and (3) page-153 is as under:
- Any indication (other than mentioned in (1)) are always acceptable in any job thickness.
- Any one and only one indication in 6t of weld length having size upto 2/3t is acceptable, for example, if t=60 mm the allowable size (diameter or other maximum dimension) of defect is 40mm.
- Now the third case is that if more than one indications within acceptable limits exist in line (we are also confused about the word "in line" as we under stand it mean that any indication touching a common straight line and the indication itself may have a maximum dimension at and oblique angle to the weld axis or may be at right angle to the weld axis), in 6t of weld length, then sum of all these indication shall not be more than t.
- But if more than one indications appear in line and the space between these indications is not greater than 3L, where L is the length of the longest indication, then length of all the indications will be summed and the sum should not be greater than 19 mm. We are also confused with "L". Kindly clarify it. Is it like the L given in FIG. 4-2 on page 355 of ASME 2001, Section VIII division 1?
- Also if any one indication having space more than 3L, but having greatest dimension more than 19 mm shall be unacceptable.
- Some of us think that if there is a indication of diameter 40 mm in a 60 mm thick job is acceptable as per Para (c) (3) of UW-52.
It will be very kind of you if all the above mentioned confusions could be cleared by examples and figures.
With regards.
Zaheer Ahmad.




 
 Reply 
 
prashant lode
prashant lode
02:26 Jan-21-2004
Re: ASME Standard for spot Radiography
----------- Start Original Message -----------
:
: Dear Sir,
: Last week we were discussing in a training course, the acceptance criteria of radiographic testing given in ASME 2001, section VIII Division 1 UW-52 for spot radiography.
: Our interpretation of Para UW-52 (c) (2) and (3) page-153 is as under:
: - Any indication (other than mentioned in (1)) are always acceptable in any job thickness.
: - Any one and only one indication in 6t of weld length having size upto 2/3t is acceptable, for example, if t=60 mm the allowable size (diameter or other maximum dimension) of defect is 40mm.
: - Now the third case is that if more than one indications within acceptable limits exist in line (we are also confused about the word "in line" as we under stand it mean that any indication touching a common straight line and the indication itself may have a maximum dimension at and oblique angle to the weld axis or may be at right angle to the weld axis), in 6t of weld length, then sum of all these indication shall not be more than t.
: - But if more than one indications appear in line and the space between these indications is not greater than 3L, where L is the length of the longest indication, then length of all the indications will be summed and the sum should not be greater than 19 mm. We are also confused with "L". Kindly clarify it. Is it like the L given in FIG. 4-2 on page 355 of ASME 2001, Section VIII division 1?
: - Also if any one indication having space more than 3L, but having greatest dimension more than 19 mm shall be unacceptable.
: - Some of us think that if there is a indication of diameter 40 mm in a 60 mm thick job is acceptable as per Para (c) (3) of UW-52.
: It will be very kind of you if all the above mentioned confusions could be cleared by examples and figures.
: With regards.
: Zaheer Ahmad.
:
------------ End Original Message ------------

dear sir,
our Klenzaids group of companies involved in the manufacturing of pressure vessel. so i need asme standard. so plz send this on my e-mail



 
 Reply 
 
Sasaki
Sasaki
08:19 Jan-22-2004
Re: ASME Standard for spot Radiography
I think your interpretation is correct.

I have not ASME-2001 by my side now, but as far as I remenber that UW52 specifies only "rounded" indication as acceptable discontinuity in non-critical joint.

As for "L", the aligned or cued indications apart each other more than "3L" can be considered as single, independent and separate, discontinuity.

Remenber that there is a definition of "rounded" indication in ASME, and "t" is not plate thickness but "weld thickness".
See the "INTERPRETATION" of the UW52 that clarifies more in detail, if any.

Interpreting the nature of "rounded" indication governs the acceptance judgement; e.g. the indication of 40 mm dia. of rounded indication will be unacceptable if it is judged incomplete fusion.

Now, I hope all is clear.

Regards,


 
 Reply 
 

Product Spotlight

Panther

M2M PANTHER is a phased-array equipment designed for both desktop and industrial applications, offer
...
ing unparalleled performance in a compact unit. It combines the speed required for industrial integrated Phased-Array Ultrasound (PAUT) solutions, with the most complete set of total focusing method (TFM) imaging techniques, making it the ultimate tool for R&D and procedure qualification.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window