where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

717 views
Technical Discussions
Dik de Groot
Dik de Groot
05:43 Oct-14-1998
mpi NDT

In either Insight or Materials Evaluation in the time frame of 1996-1997 there has been an article for making cracks in a steel plate for training purposes.
However, I can not remember or locate the article.
The method was using a heat sensitive base material on which a strip was welded (spot welded). After cooling down the strip was removed and the weld grounded flush.
At the welded spot cracks were introduced. The article was good because all the materials and the method was mentioned. It was a short article, could be in NDT Basics or Back to Basics.
Can you help me locate the article.

Thanks in advance.

Dik de Groot


 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 617

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
617
08:39 Oct-14-1998
Re: mpi NDT
: In either Insight or Materials Evaluation in the time frame of 1996-1997 there has been an article for making cracks in a steel plate for training purposes.
: However, I can not remember or locate the article.
: The method was using a heat sensitive base material on which a strip was welded (spot welded). After cooling down the strip was removed and the weld grounded flush.
: At the welded spot cracks were introduced. The article was good because all the materials and the method was mentioned. It was a short article, could be in NDT Basics or Back to Basics.
: Can you help me locate the article.

: Thanks in advance.

: Dik de Groot
-----------------
It was published in 5 parts in Insight.
For the first two issues we have the TOC's on NDTnet.
(Insight maybe continue the other issues on their own homepage
http://www.powertech.co.uk/bindt/, unfortunalty
the server is not responding)

Vol 40 No. 1 (Jan 98)
NDT FUNDAMENTALS: Magnetic Particle Testing pp. 53
www.ndt.net/bibliog/insi0198.htm

Vol 40 No. 2 (Feb 98)
Part 2. Electromagnetic induction pp. 122
www.ndt.net/bibliog/insi0298.htm

Vol 40 No. 3 (Mar 98)
Part 3. The magnetic flow method pp. 220

Vol 40 No. 4 (April 98)
Part 4. Test values pp. 292

Vol 40 No. 5 (May 98)
Part 5. Magnetic Particle inks and powers pp. 356



 
 Reply 
 
William Avrin, San Diego, CA
William Avrin, San Diego, CA
00:16 Feb-19-1999
Re: mpi NDT
I read with interest your response to a question about magnetic particle inspection of cracks in steel plates. I have been working on ultralow-frequency eddy-current methods which can potentially detect flaws several millimeters deep in steel. Can you suggest any situations where this kind of capability might be useful?


 
 Reply 
 

Product Spotlight

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>