acceptance criteria of PMI

Dear Experts,
in some PMI reports i found a comment written in bottom side----the measured value of alloying elements shall be within 10 percent of the specified level------from where this tolerance has been taken? is it mentioned in code anywhere?

 
 Reply 
 
Abderrahmane Gaouas
NDT Inspector, - sgs
sgs, Algeria, Joined Jun 2010, 9

Abderrahmane Gaouas

NDT Inspector, - sgs
sgs,
Algeria,
Joined Jun 2010
9
12:34 May-12-2016
Re: acceptance criteria of PMI
In Reply to vivek at 15:13 May-09-2016 (Opening).

For acceptance criteria of PMI, it shall be demonstrated that materials contain the amount of alloying elements shown in the material specification. Alloys shall be deemed acceptable if the alloying elements are each within ten percent (10%) of the values.
Welds having consumable material content that matches, or nearly matches, the base metal composition within approximately twelve and half percent (± 12.5%) of the ranges allowed in ASME Section II, Part C for each element.
Acceptance criteria for dissimilar metal alloy welds shall be in accordance with the welding consumable material specified in the approved welding procedure. The effects of dilution between the different base metals and the filler metal shall be taken into account when determining the nominal as-deposited weld metal composition.

 
 Reply 
 

Product Spotlight

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window