What is PMI

Dear sir:
Can you tell what is PMI (positive material identification )? Is it test method or Certificate¡K¡K¡K¡K¡K¡K¡K¡KIf PMI is Cert. ? how to apply ? and which organization can improve?
If PMI is Test method. What is this test?

Because I have buyer who want l have certified PMI for 310stainless product, but l do not know what is PMI
Please Help me?
Best regard.
Chris




 
 Reply 
 
Sasaki
Sasaki
03:56 Feb-10-2004
Re: What is PMI
Please see here.

http://www.metorex.fi/

The product name is "ARC-MET".


 
 Reply 
 
S.V.Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S.V.Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
05:55 Feb-16-2004
Re: What is PMI
Dear Chris,

PMI stands for Positive Material Identification. It is increasingly being asked for by customers on products leaving factory of the supplier or in case of receipt from warehouses, through traders etc., at the place of receipt before futher processing. There are several methods for carrying out PMI, including Spectrographic analysis, X-ray Fluorescene Analysis etc.

In case of your specific application, a Vacuum Emission Spectrometer or an Argon Flushed Spectrometer should be the right choice since you need to analyse and demonstrate all elements including Carbon, Phosphorous, Sulphur, Chromium, Nickel etc.

There are agencies providing such services so that we don't need to buy the equipment ourselves.

Swamy
India

----------- Start Original Message -----------
: Dear sir:
: Can you tell what is PMI (positive material identification )? Is it test method or Certificate¡K¡K¡K¡K¡K¡K¡K¡KIf PMI is Cert. ? how to apply ? and which organization can improve?
: If PMI is Test method. What is this test?
:
: Because I have buyer who want l have certified PMI for 310stainless product, but l do not know what is PMI
: Please Help me?
: Best regard.
: Chris
:
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Semi-Automated Phased Array Immersion System for Small Composite Parts

Turn-key semi-automated system as an improved and affordable solution for inspection of small comp
...
osite parts. Includes support table, immersion tank, scanner, PA instrument, PC, Analysis software, database, wedge management and other options.
>

GUL Subsea Solutions - Screeening & Monitoring

To inspect new and existing subsea lines, you need proven technology and experience. GUL offers it's
...
technology to solve this challenge: GUL Subsea and gMAT Transducer Rings.
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>