670 views
Technical Discussions
Dale Thorpe
Dale Thorpe
05:33 Feb-20-1999
Immersion Tank - Rust Control

We are a high volume inspection company examining automotive air bag components using robitic immersion (UT) techniques. The industry is quickly moving from aluminum to steel components.

I would appreciate any information or suggestions on a water based additive for raw uncoated steel for the immersion tanks that does not leave any oily residue or foaming properties and of course, environmental friendly.

Dale Thorpe
Advanced Material Solutions, Inc.


 
 Reply 
 
Tom Colter
Engineering,
Bechtel Plant Machinery Inc., USA, Joined Nov 1998, 3

Tom Colter

Engineering,
Bechtel Plant Machinery Inc.,
USA,
Joined Nov 1998
3
03:11 Feb-21-1999
Re: Immersion Tank - Rust Control
: We are a high volume inspection company examining automotive air bag components using robitic immersion (UT) techniques. The industry is quickly moving from aluminum to steel components.

: I would appreciate any information or suggestions on a water based additive for raw uncoated steel for the immersion tanks that does not leave any oily residue or foaming properties and of course, environmental friendly.

We have had good results using immersion tank additives from Sonotech, Inc.
http://www.sonotech-inc.com/


: Dale Thorpe
: Advanced Material Solutions, Inc.




 
 Reply 
 
Robert A. Day
Engineering
Milky Way Jewels, USA, Joined Nov 1998, 40

Robert A. Day

Engineering
Milky Way Jewels,
USA,
Joined Nov 1998
40
09:13 Feb-22-1999
Re: Immersion Tank - Rust Control
is quickly moving from aluminum to steel components.

: I would appreciate any information or suggestions on a water based additive for raw uncoated steel for the immersion tanks that does not leave any oily residue or foaming properties and of course, environmental friendly.

: Dale Thorpe
: Advanced Material Solutions, Inc.




 
 Reply 
 

Product Spotlight

New PHAsis module for longitudinal weld seam inspection

PHAsis® Phased Array manual ultrasonic spot weld inspection device is now ideally suited for test
...
ing of longitudinally welded seams (e.g. Arplas® seam, short line seams) with a length of 3 to 12 mm.
>

Semi-Automated Phased Array Immersion System for Small Composite Parts

Turn-key semi-automated system as an improved and affordable solution for inspection of small comp
...
osite parts. Includes support table, immersion tank, scanner, PA instrument, PC, Analysis software, database, wedge management and other options.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window