What is PMI

Dear sir:
Can you tell what is PMI (positive material identification )? Is it test method or Certificate¡K¡K¡K¡K¡K¡K¡K¡KIf PMI is Cert. ? how to apply ? and which organization can improve?
If PMI is Test method. What is this test?

Because I have buyer who want l have certified PMI for 310stainless product, but l do not know what is PMI
Please Help me?
Best regard.
Chris




 
 Reply 
 
Sasaki
Sasaki
03:56 Feb-10-2004
Re: What is PMI
Please see here.

http://www.metorex.fi/

The product name is "ARC-MET".


 
 Reply 
 
S.V.Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S.V.Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
05:55 Feb-16-2004
Re: What is PMI
Dear Chris,

PMI stands for Positive Material Identification. It is increasingly being asked for by customers on products leaving factory of the supplier or in case of receipt from warehouses, through traders etc., at the place of receipt before futher processing. There are several methods for carrying out PMI, including Spectrographic analysis, X-ray Fluorescene Analysis etc.

In case of your specific application, a Vacuum Emission Spectrometer or an Argon Flushed Spectrometer should be the right choice since you need to analyse and demonstrate all elements including Carbon, Phosphorous, Sulphur, Chromium, Nickel etc.

There are agencies providing such services so that we don't need to buy the equipment ourselves.

Swamy
India

----------- Start Original Message -----------
: Dear sir:
: Can you tell what is PMI (positive material identification )? Is it test method or Certificate¡K¡K¡K¡K¡K¡K¡K¡KIf PMI is Cert. ? how to apply ? and which organization can improve?
: If PMI is Test method. What is this test?
:
: Because I have buyer who want l have certified PMI for 310stainless product, but l do not know what is PMI
: Please Help me?
: Best regard.
: Chris
:
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window