Jean-Pascal Reymondin
Jean-Pascal Reymondin
06:50 Feb-13-2004
Detection of small nonmetallic inclusion

Does anybody know how to detect small non metalic inclusion ( 0,010 mm to 0,020 mm ) into steel ( X51CrMo3 or X51CrMoV5-1 ).
Steel thickness 0,5 mm
Détection on the surface and in the volume.

Thank you


 
 Reply 
 
Jim Kovarik
Jim Kovarik
06:19 Feb-19-2004
Re: Detection of small nonmetallic inclusion
----------- Start Original Message -----------
: Does anybody know how to detect small non metalic inclusion ( 0,010 mm to 0,020 mm ) into steel ( X51CrMo3 or X51CrMoV5-1 ).
: Steel thickness 0,5 mm
: Détection on the surface and in the volume.
: Thank you
------------ End Original Message ------------

A radiographic linear array system should be able to detect these indications.
Lixi Inc. has some experience with these systems. Their website is www.lixi.com


 
 Reply 
 
Francois Blanchard
Francois Blanchard
06:27 Feb-19-2004
Re: Detection of small nonmetallic inclusion
----------- Start Original Message -----------
: Does anybody know how to detect small non metalic inclusion ( 0,010 mm to 0,020 mm ) into steel ( X51CrMo3 or X51CrMoV5-1 ).
: Steel thickness 0,5 mm
: Détection on the surface and in the volume.
: Thank you
------------ End Original Message ------------

You can also investigate the possibility of a laser ultrasonic system. Expensive but able to detect high frequency ultrasound. (www.tecnar.com) With Ghz ultrasound, I was able to measured thickness foil down to 10um.
regards,
Francois




 
 Reply 
 
John Pursley
R & D
Envision Product Design, USA, Joined Oct 1999, 23

John Pursley

R & D
Envision Product Design,
USA,
Joined Oct 1999
23
00:06 Feb-20-2004
Re: Detection of small nonmetallic inclusion
Envision's high resolution digital X-ray panels and linear arrays along with a micro-focus source will image your inclusions in the 10 to 20 micron range. http://cmosxray.com

----------- Start Original Message -----------
: : Does anybody know how to detect small non metalic inclusion ( 0,010 mm to 0,020 mm ) into steel ( X51CrMo3 or X51CrMoV5-1 ).
: : Steel thickness 0,5 mm
: : Détection on the surface and in the volume.
: : Thank you
: You can also investigate the possibility of a laser ultrasonic system. Expensive but able to detect high frequency ultrasound. (www.tecnar.com) With Ghz ultrasound, I was able to measured thickness foil down to 10um.
: regards,
: Francois
------------ End Original Message ------------




 
 Reply 
 
rizal
rizal
01:03 Feb-24-2004
Re: Detection of small nonmetallic inclusion
please comment and give some tips about my research.. topic:
Investigation of crack defect in roof clay product using ultrasonic
machine
thanks alot..



 
 Reply 
 
Zhong Soo Lim
Zhong Soo Lim
01:40 Apr-15-2004
Re: Detection of small nonmetallic inclusion
----------- Start Original Message -----------
: Does anybody know how to detect small non metalic inclusion ( 0,010 mm to 0,020 mm ) into steel ( X51CrMo3 or X51CrMoV5-1 ).
: Steel thickness 0,5 mm
: Détection on the surface and in the volume.
: Thank you
------------ End Original Message ------------

Magnetic Leakage Flux method can be one of the possible candidates, which is good since it is a noncontact method, and no couplant is needed.
I have done a similar research, which is very easy to apply.
The detectivity of the nonmetallic inclusion can be down to 1x10^(-4) mm^(3), or better than that in some cases.
There can be some limitations.

1. Surface condition
2. Uniformity of the inner material structure

The thickness of 0.5 mm can be a problem.
But you can access from both sides (top and bottom).

If you have any question, then we can discuss further.

Zhong Soo Lim



 
 Reply 
 

Product Spotlight

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

On Demand Webinar: Improve the Efficiency and Accuracy of Inspection Scanning

On-demand webinar on scanning technology that helps improve the efficiency and accuracy of ultrasoni
...
c inspections in oil and gas, aerospace, manufacturing and other industrial applications. The webinar features a scanning solution for multiple inspection environments, including flat and curved specimens, magnetic and nonmagnetic surfaces and raster scanning over long distances. View it today.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window