Immersion Tank - Rust Control

We are a high volume inspection company examining automotive air bag components using robitic immersion (UT) techniques. The industry is quickly moving from aluminum to steel components.

I would appreciate any information or suggestions on a water based additive for raw uncoated steel for the immersion tanks that does not leave any oily residue or foaming properties and of course, environmental friendly.

Dale Thorpe
Advanced Material Solutions, Inc.


 
 Reply 
 
Tom Colter
Engineering,
Bechtel Plant Machinery Inc., USA, Joined Nov 1998, 3

Tom Colter

Engineering,
Bechtel Plant Machinery Inc.,
USA,
Joined Nov 1998
3
03:11 Feb-21-1999
Re: Immersion Tank - Rust Control
: We are a high volume inspection company examining automotive air bag components using robitic immersion (UT) techniques. The industry is quickly moving from aluminum to steel components.

: I would appreciate any information or suggestions on a water based additive for raw uncoated steel for the immersion tanks that does not leave any oily residue or foaming properties and of course, environmental friendly.

We have had good results using immersion tank additives from Sonotech, Inc.
http://www.sonotech-inc.com/


: Dale Thorpe
: Advanced Material Solutions, Inc.




 
 Reply 
 
Robert A. Day
Engineering
Milky Way Jewels, USA, Joined Nov 1998, 40

Robert A. Day

Engineering
Milky Way Jewels,
USA,
Joined Nov 1998
40
09:13 Feb-22-1999
Re: Immersion Tank - Rust Control
is quickly moving from aluminum to steel components.

: I would appreciate any information or suggestions on a water based additive for raw uncoated steel for the immersion tanks that does not leave any oily residue or foaming properties and of course, environmental friendly.

: Dale Thorpe
: Advanced Material Solutions, Inc.




 
 Reply 
 

Product Spotlight

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window