where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

927 views
Technical Discussions
Velu Perumal
Consultant, Research
National University of Singapore ,Singapore, Singapore, Joined Jun 2003, 1

Velu Perumal

Consultant, Research
National University of Singapore ,Singapore,
Singapore,
Joined Jun 2003
1
05:39 Aug-26-2003
Detecting thermal crack by NDT methods

Dear All,
I am working on thermal cracks on concrete.I would like to measure thermal stress and strains,crack precisely.Ofcourse surface cracks we can measure any methods. But thermal cracks are haapened internally.Can i measure thermal cracks using any one of current NDT methods.We already conducted thermal shock experiment (Circular Ring Specimen) using AE. Currently we have Acoustic Emmission(AE),UPV & Impact echo.please give your valuable suggestions


 
 Reply 
 
Bastiaan Janssen
NDT Inspector, Managing Xray micro-Tomography
NRG, Netherlands, Joined Jul 2003, 4

Bastiaan Janssen

NDT Inspector, Managing Xray micro-Tomography
NRG,
Netherlands,
Joined Jul 2003
4
03:13 Aug-27-2003
Re: Detecting thermal crack by NDT methods
Dear Velu Perumal,

Depending on size of test samples, erg. drilled core cylinders, I would suggest micro tomography,.Using x-ray or gamma ray's and a focal spot for the radiation source, this results in magnified projections wich can be reconstructed, using using many pictures form differend angeles, into a 3D-dataset. We have obtained internal crack visualisations of concrete cylinders diameter 5 cm, with a resolution of 1/10 m; Depending on x-ray energy, source spotsize and sample diameter...

Best regards.
(On holliday until october)
http://www.nrg-nl.com/product/ppt/tomo/index.html

----------- Start Original Message -----------
: Dear All,
: I am working on thermal cracks on concrete.I would like to measure thermal stress and strains,crack precisely.Ofcourse surface cracks we can measure any methods. But thermal cracks are haapened internally.Can i measure thermal cracks using any one of current NDT methods.We already conducted thermal shock experiment (Circular Ring Specimen) using AE. Currently we have Acoustic Emmission(AE),UPV & Impact echo.please give your valuable suggestions
------------ End Original Message ------------




 
 Reply 
 
R.Malathy, Senior Lecturer in Civil Engineering, Kongu Engineering college, Peru
R.Malathy, Senior Lecturer in Civil Engineering, Kongu Engineering college, Peru
09:32 Feb-26-2004
Re: Detecting thermal crack by NDT methods
Dear Sir,

We have TICO ultrasonic Pulse velocity tester. How to measure the thermal cracks.


 
 Reply 
 
zuhudruba
zuhudruba
03:17 Apr-08-2005
Re: Detecting thermal crack by NDT methods
----------- Start Original Message -----------
: Dear All,
: I am working on thermal cracks on concrete.I would like to measure thermal stress and strains,crack precisely.Ofcourse surface cracks we can measure any methods. But thermal cracks are haapened internally.Can i measure thermal cracks using any one of current NDT methods.We already conducted thermal shock experiment (Circular Ring Specimen) using AE. Currently we have Acoustic Emmission(AE),UPV & Impact echo.please give your valuable suggestions
------------ End Original Message ------------




 
 Reply 
 
TERD
TERD
08:21 Jul-03-2005
Re: Detecting thermal crack by NDT methods
----------- Start Original Message -----------
: Dear Velu Perumal,
: Depending on size of test samples, erg. drilled core cylinders, I would suggest micro tomography,.Using x-ray or gamma ray's and a focal spot for the radiation source, this results in magnified projections wich can be reconstructed, using using many pictures form differend angeles, into a 3D-dataset. We have obtained internal crack visualisations of concrete cylinders diameter 5 cm, with a resolution of 1/10 m; Depending on x-ray energy, source spotsize and sample diameter...
: Best regards.
: (On holliday until october)
: http://www.nrg-nl.com/product/ppt/tomo/index.html
: : Dear All,
: : I am working on thermal cracks on concrete.I would like to measure thermal stress and strains,crack precisely.Ofcourse surface cracks we can measure any methods. But thermal cracks are haapened internally.Can i measure thermal cracks using any one of current NDT methods.We already conducted thermal shock experiment (Circular Ring Specimen) using AE. Currently we have Acoustic Emmission(AE),UPV & Impact echo.please give your valuable suggestions
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window