Dear Experts,

can you suggest what will be the frequency(T/R-Probe) of probe use for 3 mm wall thickness ,check for lamination.

 
 Reply 
 
dhiliban
Other, QA/QC engineer
L&T HCP, India, Joined May 2016, 16

dhiliban

Other, QA/QC engineer
L&T HCP,
India,
Joined May 2016
16
10:00 Jul-08-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

Use:-4-5 MHZ probes


The sensitivity of the probe is directly proprtional to its frequency
and The depth of penetration is inversely proportional to frequency

So if you use a probe with higher frequency you will have better sensitivity,since your thickness is less,depth of penetration wont be a problem.


With regards,
Dhiliban.

 
 Reply 
 
massimo carminati
Consultant, AUT specialist
IMG Ultrasuoni Srl, Italy, Joined Apr 2007, 691

massimo carminati

Consultant, AUT specialist
IMG Ultrasuoni Srl,
Italy,
Joined Apr 2007
691
07:07 Jul-10-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

I would use a 10 MHz short focus dual probe. If you don't know where to afford it, feel free to contact me directly

 
 Reply 
 
ismail
NDT Inspector, TOFD and PAUT Specialist
Turkey, Joined Oct 2008, 27

ismail

NDT Inspector, TOFD and PAUT Specialist
Turkey,
Joined Oct 2008
27
10:27 Jul-10-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

I recommend to 15 MHz Delay line probe
Ismail

 
 Reply 
 
Kevin Humphreys
Kevin Humphreys
11:19 Jul-11-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

A dual 10 MHz should suffice

 
 Reply 
 
Darren Quinn
Darren Quinn
06:30 Jul-14-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

I am going with 10 MHZ here 6mm diameter short focus :)

 
 Reply 
 

Product Spotlight

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>