umeshkumar
umeshkumar
07:15 Jul-08-2016
for thickness 03 mm ,lamination check

Dear Experts,

can you suggest what will be the frequency(T/R-Probe) of probe use for 3 mm wall thickness ,check for lamination.

 
 Reply 
 
dhiliban
Other, QA/QC engineer
L&T HCP, India, Joined May 2016, 16

dhiliban

Other, QA/QC engineer
L&T HCP,
India,
Joined May 2016
16
10:00 Jul-08-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

Use:-4-5 MHZ probes


The sensitivity of the probe is directly proprtional to its frequency
and The depth of penetration is inversely proportional to frequency

So if you use a probe with higher frequency you will have better sensitivity,since your thickness is less,depth of penetration wont be a problem.


With regards,
Dhiliban.

 
 Reply 
 
massimo carminati
Consultant, AUT specialist
IMG Ultrasuoni Srl, Italy, Joined Apr 2007, 691

massimo carminati

Consultant, AUT specialist
IMG Ultrasuoni Srl,
Italy,
Joined Apr 2007
691
07:07 Jul-10-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

I would use a 10 MHz short focus dual probe. If you don't know where to afford it, feel free to contact me directly

 
 Reply 
 
ismail
NDT Inspector, TOFD and PAUT Specialist
Turkey, Joined Oct 2008, 24

ismail

NDT Inspector, TOFD and PAUT Specialist
Turkey,
Joined Oct 2008
24
10:27 Jul-10-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

I recommend to 15 MHz Delay line probe
Ismail

 
 Reply 
 
Kevin Humphreys
Kevin Humphreys
11:19 Jul-11-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

A dual 10 MHz should suffice

 
 Reply 
 
Darren Quinn
Darren Quinn
06:30 Jul-14-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

I am going with 10 MHZ here 6mm diameter short focus :)

 
 Reply 
 

Product Spotlight

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

High-end Ultrasonic Flaw Detector with 32:128PR PAUT and 2-ch TOFD: SyncScan 2

SIUI’s newly launched SyncScan 2, is a high-end ultrasonic flaw detector with 32:128PR PAUT and
...
2-ch TOFD, which can maximize your efficiency for PA and TOFD. ● Support PA/TOFD/UT ● 32-ch PA is more suitable for inspection on extra-thick wall and high-attenuation material. ● 32-ch PA and 2-ch TOFD work simultaneously. ● Support PR mode for corrosion inspection.
>

Magnetic X-Ray Pipeline Crawler

Zhong Yi brand pipeline crawler is magnetic/micro-video controlled crawler with DC X ray unit inst
...
alled for checking welding of pipeline. Move steadily inside the pipeline 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometers and provide the efficient inspection of the pipeline.
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window