umeshkumar
umeshkumar
07:15 Jul-08-2016
for thickness 03 mm ,lamination check

Dear Experts,

can you suggest what will be the frequency(T/R-Probe) of probe use for 3 mm wall thickness ,check for lamination.

 
 Reply 
 
dhiliban
Other, QA/QC engineer
L&T HCP, India, Joined May 2016, 16

dhiliban

Other, QA/QC engineer
L&T HCP,
India,
Joined May 2016
16
10:00 Jul-08-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

Use:-4-5 MHZ probes


The sensitivity of the probe is directly proprtional to its frequency
and The depth of penetration is inversely proportional to frequency

So if you use a probe with higher frequency you will have better sensitivity,since your thickness is less,depth of penetration wont be a problem.


With regards,
Dhiliban.

 
 Reply 
 
massimo carminati
Consultant, AUT specialist
IMG Ultrasuoni Srl, Italy, Joined Apr 2007, 691

massimo carminati

Consultant, AUT specialist
IMG Ultrasuoni Srl,
Italy,
Joined Apr 2007
691
07:07 Jul-10-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

I would use a 10 MHz short focus dual probe. If you don't know where to afford it, feel free to contact me directly

 
 Reply 
 
ismail
NDT Inspector, TOFD and PAUT Specialist
Turkey, Joined Oct 2008, 27

ismail

NDT Inspector, TOFD and PAUT Specialist
Turkey,
Joined Oct 2008
27
10:27 Jul-10-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

I recommend to 15 MHz Delay line probe
Ismail

 
 Reply 
 
Kevin Humphreys
Kevin Humphreys
11:19 Jul-11-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

A dual 10 MHz should suffice

 
 Reply 
 
Darren Quinn
Darren Quinn
06:30 Jul-14-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

I am going with 10 MHZ here 6mm diameter short focus :)

 
 Reply 
 

Product Spotlight

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>