where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

1247 views
Technical Discussions
umeshkumar
umeshkumar
07:15 Jul-08-2016
for thickness 03 mm ,lamination check

Dear Experts,

can you suggest what will be the frequency(T/R-Probe) of probe use for 3 mm wall thickness ,check for lamination.

 
 Reply 
 
dhiliban
Other, QA/QC engineer
L&T HCP, India, Joined May 2016, 16

dhiliban

Other, QA/QC engineer
L&T HCP,
India,
Joined May 2016
16
10:00 Jul-08-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

Use:-4-5 MHZ probes


The sensitivity of the probe is directly proprtional to its frequency
and The depth of penetration is inversely proportional to frequency

So if you use a probe with higher frequency you will have better sensitivity,since your thickness is less,depth of penetration wont be a problem.


With regards,
Dhiliban.

 
 Reply 
 
massimo carminati
Consultant, AUT specialist
IMG Ultrasuoni Srl, Italy, Joined Apr 2007, 691

massimo carminati

Consultant, AUT specialist
IMG Ultrasuoni Srl,
Italy,
Joined Apr 2007
691
07:07 Jul-10-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

I would use a 10 MHz short focus dual probe. If you don't know where to afford it, feel free to contact me directly

 
 Reply 
 
ismail
NDT Inspector, TOFD and PAUT Specialist
Turkey, Joined Oct 2008, 27

ismail

NDT Inspector, TOFD and PAUT Specialist
Turkey,
Joined Oct 2008
27
10:27 Jul-10-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

I recommend to 15 MHz Delay line probe
Ismail

 
 Reply 
 
Kevin Humphreys
Kevin Humphreys
11:19 Jul-11-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

A dual 10 MHz should suffice

 
 Reply 
 
Darren Quinn
Darren Quinn
06:30 Jul-14-2016
Re: for thickness 03 mm ,lamination check
In Reply to umeshkumar at 07:15 Jul-08-2016 (Opening).

I am going with 10 MHZ here 6mm diameter short focus :)

 
 Reply 
 

Product Spotlight

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Portable Ground Penetrating Radar - Proceq GP8000

The Proceq GP8000 portable ground penetrating radar instrument is the beginning of a new era in ND
...
T. The outstanding, patented ultra- wideband technology combined with a compact wireless probe delivers unmatched industry performance. Proceq GP8000 is the world’s first large-scale inspection solution that utilizes Augmented Reality in industrial applications.
>

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>