Ehssein
Ehssein
05:39 Feb-02-2004
AT quartz cut

Dear all, I have searched it and I didn't find: what does the appreviation AT means in "AT quartz cut"
Thank you in advance.


 
 Reply 
 
Nick Welland
Nick Welland
01:36 Feb-03-2004
Re: AT quartz cut
----------- Start Original Message -----------
: Dear all, I have searched it and I didn't find: what does the appreviation AT means in "AT quartz cut"
: Thank you in advance.
------------ End Original Message ------------
The "T" means it is a temperature-compensated cut; the orientation is such as to cancel out positive and negative temperature coefficients affecting the vibration frequency, The "A" means it was the first such cut discovered. From memory, the plate is cut parallel to the X crystallographic axis, and inclined at about 35 deg to the Z axis. Quartz is very anisotropic in its properties and there different cuts for various purposes.
Best regards
Nick



 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1292

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1292
03:57 Feb-26-2004
Re: AT quartz cut

Nick: what a good memory you have! The AT cut is indeed 35 degrees from the Z-axis (but parallel to the Y-cut).
I recalled the various cuts being illustrated in an old book I had as an optical mineralogy student, Elements of Mineralogy, by B.Mason and L. Berry, Published by W H Freeman and company, 1968.
I have scanned Figure 4.5 from that text to illustrate the various cuts of oscillator plates that have been cut from quartz crystals.

http://www.ndt.net/wshop/attach/quartz.gif

The quartz crystal was first noted as having piezoelectric properties in 1881 (brothers Curie) but had no applications outside the lab until about 1915 when sonar development began. Later it held importance in radio tuners. Here it waw used with an alternating electrical field applied across the quartz plate. When suitably cut and mounted and dimensioned so that one of its natural frequencies of mechanical vibration matched the resonant frequency of the electrical circuit, the frequency of transmission or receptionwas stabilised or controlled.


----------- Start Original Message -----------
: : Dear all, I have searched it and I didn't find: what does the appreviation AT means in "AT quartz cut"
: : Thank you in advance.
: The "T" means it is a temperature-compensated cut; the orientation is such as to cancel out positive and negative temperature coefficients affecting the vibration frequency, The "A" means it was the first such cut discovered. From memory, the plate is cut parallel to the X crystallographic axis, and inclined at about 35 deg to the Z axis. Quartz is very anisotropic in its properties and there different cuts for various purposes.
: Best regards
: Nick
------------ End Original Message ------------




 
 Reply 
 
Nick Welland
Nick Welland
08:09 Feb-28-2004
Re: AT quartz cut
----------- Start Original Message -----------
: Nick: what a good memory you have! The AT cut is indeed 35 degrees from the Z-axis (but parallel to the Y-cut).
: I recalled the various cuts being illustrated in an old book I had as an optical mineralogy student, Elements of Mineralogy, by B.Mason and L. Berry, Published by W H Freeman and company, 1968.
: I have scanned Figure 4.5 from that text to illustrate the various cuts of oscillator plates that have been cut from quartz crystals.
: http://www.ndt.net/wshop/attach/quartz.gif
: The quartz crystal was first noted as having piezoelectric properties in 1881 (brothers Curie) but had no applications outside the lab until about 1915 when sonar development began. Later it held importance in radio tuners. Here it waw used with an alternating electrical field applied across the quartz plate. When suitably cut and mounted and dimensioned so that one of its natural frequencies of mechanical vibration matched the resonant frequency of the electrical circuit, the frequency of transmission or reception was stabilised or controlled.
:
: : : Dear all, I have searched it and I didn't find: what does the appreviation AT means in "AT quartz cut"
: : : Thank you in advance.
: : The "T" means it is a temperature-compensated cut; the orientation is such as to cancel out positive and negative temperature coefficients affecting the vibration frequency, The "A" means it was the first such cut discovered. From memory, the plate is cut parallel to the X crystallographic axis, and inclined at about 35 deg to the Z axis. Quartz is very anisotropic in its properties and there different cuts for various purposes.
: : Best regards
: : Nick
------------ End Original Message ------------
As always, Ed, your scholarship amazes me. Thanks for the memories! (My text was Kerr's Optical Mineralogy)
Nick


 
 Reply 
 

Product Spotlight

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

GEKKO, Standard and Advanced phased-array for Easier inspection

M2M Gekko® is a field-proven flaw detector offering PAUT, UT, TOFD and TFM through the streamline
...
d user interface Capture™. Released in 32:128, 64:64 or 64:128 channel configurations, Gekko combines high- resolution and speed while reducing inspectors’ training time.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window