Greeting ,
I am in the process of start the PAUT on the piping weld joint to replace RT, basically pipe size range from 1” to 36” and all the size have the sch40,80,120and 160 plus some special thickness.
I propose the pipe size for PAUT from 4” and above.I have both P1 and P8 material and some other special material also.
As per ASME sec V T-434.3 piping calibration block is required same nominal size and schedule.
I required your advice that
1. Can we take the benefit of curvature from 0.9 to 1.5 times the basic calibration block diameter for the curvature as per ASME Sec V T-434.1.7.2?
2. How about the different pipe Sch ? Is it required separate calibration block for pipe every different SCH with same pipe diameter?(e.g 8” pipe with S40,S80,S120 etc)
please advice ,for your information I am sending the list of pipe size required to phase array please give some advice to minimize the no of calibration block to cover the all pipe size.

BHASKAR KALE
bmkale@gmail.com

 
 Reply 
 
Nguyen Trong My
Director,
Vietnam Inspection Solutions Co., Ltd, Vietnam, Joined May 2000, 22

Nguyen Trong My

Director,
Vietnam Inspection Solutions Co., Ltd,
Vietnam,
Joined May 2000
22
16:24 Mar-08-2011
Re: PAUT Calibration Block
In Reply to BHASKAR KALE at 03:59 Mar-07-2011 (Opening).

Hello BHASKAR,
1. For pipe size from 1" to 4 " you can also use PAUT using small-diameter pipe scanners, such as COBRA SCANNER of Olympus NDT or BRACELET of Phoenix etc.
2. You can take the benefit of Code case 2638 Alternative Piping Calibration Blocks for UT to prepare your calibration blocks. Now the same tolerances and range on block curvature as for vessel welds are allowed, see Fig.-434.1.7.2. Additionally thickness, T, may be + / - 25% of the component thickness (see "ASME CALIBRATION BLOCK FOR PIPING " messages of Nigel et al. in this forum).
Nguyen Trong My

 
 Reply 
 
BHASKAR KALE
BHASKAR KALE
01:50 Mar-09-2011
Re: PAUT Calibration Block
In Reply to Nguyen Trong My at 16:24 Mar-08-2011 .

Thank you very much, much appreciate your swift replay and now clear all my concern and really now i can save lot of work and cost.
Bhaskar

 
 Reply 
 
jacky
jacky
05:33 Aug-08-2016
Re: PAUT Calibration Block
In Reply to Nguyen Trong My at 16:24 Mar-08-2011 .

hello,

I want to know what kind of block you use for wedge delay, sensitivity calibration, because for piping inspection our wedge is curvture, so our block should not be flat.

please advice us, we have same job too.

regards
jacky

 
 Reply 
 
Andrew Brewis
Andrew Brewis
08:50 Aug-08-2016
Re: PAUT Calibration Block
In Reply to jacky at 05:33 Aug-08-2016 .

Hi Jacky,

At Phoenix ISL we always recommend that customers perform a calibration with the wedge they are going to carry out the inspection with. This is why we manufacture a whole range of contoured calibration blocks for Phased Array which allow for Sensitivity, Velocity, Wedge Delay and also TCG calibrations. If you want further information please feel free to contact me.

Regards Andrew
abrewis@phoenixisl.com

 
 Reply 
 
Andrew Robinson
Sales,
PH Tool Reference Standards, USA, Joined Feb 2012, 5

Andrew Robinson

Sales,
PH Tool Reference Standards,
USA,
Joined Feb 2012
5
16:09 Aug-08-2016
Re: PAUT Calibration Block
In Reply to jacky at 05:33 Aug-08-2016 .

Jacky and Bhaskar,

Contoured calibration blocks for pipe inspection are also available from PH Tool in the U.S. Certified calibration blocks with curved scanning surfaces are manufactured for general equipment setup and calibration for axial or circumferential scanning. Pipe calibration blocks made in accordance with ASME Sec V requirements are also available with EDM notches and SDH reflectors. I would be happy to provide more information upon request.

Best regards,
Andrew

 
 Reply 
 
Bruno
Student,
Argentina, Joined Jun 2013, 21

Bruno

Student,
Argentina,
Joined Jun 2013
21
21:10 Aug-10-2016
Re: PAUT Calibration Block
In Reply to Andrew Robinson at 16:09 Aug-08-2016 .

Andrew, can you show some pictures of one of these blocks?

 
 Reply 
 
Andrew Robinson
Sales,
PH Tool Reference Standards, USA, Joined Feb 2012, 5

Andrew Robinson

Sales,
PH Tool Reference Standards,
USA,
Joined Feb 2012
5
21:49 Aug-12-2016
Re: PAUT Calibration Block
In Reply to Bruno at 21:10 Aug-10-2016 .

zoom image






zoom image



zoom image






Bruno,

Certainly. Please see some images attached.

Thanks,
Andrew
 
 Reply 
 
srinivas
NDT Inspector,
kalva engineers pvt ltd, India, Joined Oct 2012, 35

srinivas

NDT Inspector,
kalva engineers pvt ltd,
India,
Joined Oct 2012
35
07:29 Aug-16-2016
Re: PAUT Calibration Block
In Reply to BHASKAR KALE at 03:59 Mar-07-2011 (Opening).

sir
why dont you go for ASTM E 2491 standard

 
 Reply 
 

Product Spotlight

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window