Rastislav Milan
NDT Inspector
U.S.Steel Kosice s.r.o, Slovak Republic, Joined Aug 2002, 4

Rastislav Milan

NDT Inspector
U.S.Steel Kosice s.r.o,
Slovak Republic,
Joined Aug 2002
4
01:02 Mar-20-2004
nickel hardness

Hello everybody.
Can somebody help me with my problem? I need know reletionship between nickel hardnesses and temperature(graph or table).Can you advise me some good idea orlink URL?
Thank you.
Rastislav Milan
my adress rmilan@usske.sk


 
 Reply 
 
Ed T.
Ed T.
02:02 Mar-20-2004
Re: nickel hardness
----------- Start Original Message -----------
: Hello everybody.
: Can somebody help me with my problem? I need know reletionship between nickel hardnesses and temperature(graph or table).Can you advise me some good idea orlink URL?
: Thank you.
: Rastislav Milan
: my adress rmilan@usske.sk
------------ End Original Message ------------

Try this link: http://neon.mems.cmu.edu/rollett/27301/Hwk4.27Sep02.Strnth.ans.pdf


 
 Reply 
 

Product Spotlight

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window