01:56 Mar-20-2004
U/G condition Assessment

We have Oily water drain U/G lines that were found severly corroded and started leaking contaminating soil. These lines are C.S and externaly PE wraped. Please advise on available NDT methods that can be utilized to assess the condition of these lines without excavation.


 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1307

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1307
07:12 Mar-20-2004
Re: U/G condition Assessment
To assess the best option more details are needed.
Diameter of pipe, wall thickness, the maximum bend that migh represent restriction of instrumentation put in the line, the presence of any fittings that migh restrict access and the length of line are a few that come to mind.

I have seen a small diameter pigging tool (I think it was an RTD instrument) and Oceaneering has a good selection of ROVs that could be useful too.

----------- Start Original Message -----------
: We have Oily water drain U/G lines that were found severly corroded and started leaking contaminating soil. These lines are C.S and externaly PE wraped. Please advise on available NDT methods that can be utilized to assess the condition of these lines without excavation.
------------ End Original Message ------------




 
 Reply 
 
Gary
Consultant
TWI, United Kingdom, Joined May 2001, 15

Gary

Consultant
TWI,
United Kingdom,
Joined May 2001
15
09:35 Mar-20-2004
Re: U/G condition Assessment
----------- Start Original Message -----------
: We have Oily water drain U/G lines that were found severly corroded and started leaking contaminating soil. These lines are C.S and externaly PE wraped. Please advise on available NDT methods that can be utilized to assess the condition of these lines without excavation.
------------ End Original Message ------------

Teletest® is a novel non-invasive long range ultrasonic testing method for the rapid survey of pipes, for the detection of both internal and external corrosion. Other types of defect may also be detected.

The principal advantage is that long lengths of pipe, up to 175m (575ft) in each direction, may be examined from a single test point.

The benefits are:

Reduction in the costs of gaining access to the pipes for inspection.
Avoidance of removal and reinstatement of insulation or coatings (where present), except for the area on which the test head is mounted.
The ability to inspect inaccessible areas, such as at clamps or sleeved or buried pipes.
The whole pipe wall is tested, thereby achieving a 100% examination.





 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
08:25 Mar-21-2004
Re: U/G condition Assessment
This is one of those cases where you need a lot of details. In particular the issues over what degradation mechanism is occurring, reliability of NDE techniques to detect it and whether you need to size the damage. Access and cost become the next issues.

There are a number of techniques available.

Guided Wave UT is a screening option but effective ditance may be affected by access and the external PE coating.
Internal pigging tools will probbaly provide high quality data but you require access and they are not cheap.
There is a technique called No Pig from Germany which allows some screening with only contact at 1 km access points. Again it may not be cost effcetive.

Depending upon what you are looking at AE testing may also be able to produce effective data.

You need to consider a risk based screening approach with specific inspection selected at appropriate points.

Please contact me if you require more data.



 
 Reply 
 

Product Spotlight

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>