01:56 Mar-20-2004
U/G condition Assessment

We have Oily water drain U/G lines that were found severly corroded and started leaking contaminating soil. These lines are C.S and externaly PE wraped. Please advise on available NDT methods that can be utilized to assess the condition of these lines without excavation.


 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1307

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1307
07:12 Mar-20-2004
Re: U/G condition Assessment
To assess the best option more details are needed.
Diameter of pipe, wall thickness, the maximum bend that migh represent restriction of instrumentation put in the line, the presence of any fittings that migh restrict access and the length of line are a few that come to mind.

I have seen a small diameter pigging tool (I think it was an RTD instrument) and Oceaneering has a good selection of ROVs that could be useful too.

----------- Start Original Message -----------
: We have Oily water drain U/G lines that were found severly corroded and started leaking contaminating soil. These lines are C.S and externaly PE wraped. Please advise on available NDT methods that can be utilized to assess the condition of these lines without excavation.
------------ End Original Message ------------




 
 Reply 
 
Gary
Consultant
TWI, United Kingdom, Joined May 2001, 15

Gary

Consultant
TWI,
United Kingdom,
Joined May 2001
15
09:35 Mar-20-2004
Re: U/G condition Assessment
----------- Start Original Message -----------
: We have Oily water drain U/G lines that were found severly corroded and started leaking contaminating soil. These lines are C.S and externaly PE wraped. Please advise on available NDT methods that can be utilized to assess the condition of these lines without excavation.
------------ End Original Message ------------

Teletest® is a novel non-invasive long range ultrasonic testing method for the rapid survey of pipes, for the detection of both internal and external corrosion. Other types of defect may also be detected.

The principal advantage is that long lengths of pipe, up to 175m (575ft) in each direction, may be examined from a single test point.

The benefits are:

Reduction in the costs of gaining access to the pipes for inspection.
Avoidance of removal and reinstatement of insulation or coatings (where present), except for the area on which the test head is mounted.
The ability to inspect inaccessible areas, such as at clamps or sleeved or buried pipes.
The whole pipe wall is tested, thereby achieving a 100% examination.





 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 281

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
281
08:25 Mar-21-2004
Re: U/G condition Assessment
This is one of those cases where you need a lot of details. In particular the issues over what degradation mechanism is occurring, reliability of NDE techniques to detect it and whether you need to size the damage. Access and cost become the next issues.

There are a number of techniques available.

Guided Wave UT is a screening option but effective ditance may be affected by access and the external PE coating.
Internal pigging tools will probbaly provide high quality data but you require access and they are not cheap.
There is a technique called No Pig from Germany which allows some screening with only contact at 1 km access points. Again it may not be cost effcetive.

Depending upon what you are looking at AE testing may also be able to produce effective data.

You need to consider a risk based screening approach with specific inspection selected at appropriate points.

Please contact me if you require more data.



 
 Reply 
 

Product Spotlight

Portable Ground Penetrating Radar - Proceq GP8000

The Proceq GP8000 portable ground penetrating radar instrument is the beginning of a new era in ND
...
T. The outstanding, patented ultra- wideband technology combined with a compact wireless probe delivers unmatched industry performance. Proceq GP8000 is the world’s first large-scale inspection solution that utilizes Augmented Reality in industrial applications.
>

On Demand Webinar: Improve the Efficiency and Accuracy of Inspection Scanning

On-demand webinar on scanning technology that helps improve the efficiency and accuracy of ultrasoni
...
c inspections in oil and gas, aerospace, manufacturing and other industrial applications. The webinar features a scanning solution for multiple inspection environments, including flat and curved specimens, magnetic and nonmagnetic surfaces and raster scanning over long distances. View it today.
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window