RFEC Inspection of Cast and Ductile Iron Mains

we are researching methods to inspect and determine the degree of corrosion based upon remaining wall thickness of about 40 cast and ductile iron water and wastewater subaqueous crossings in Pinellas County Florida USA.

We are aware of Hydroscope and their service. Is there a competitor to Hydroscope in the marketplace?

Thanks,

Dana


    
 
 Reply 
 
Chris Coughlin
Chris Coughlin
03:06 Mar-25-2004
Re: RFEC Inspection of Cast and Ductile Iron Mains
Dana,

I'm not sure if they're still in the business or not but a company called TexTex out of PA did some RFEC work for us a few years ago, maybe they're worth a visit: http://www.testex-ndt.com/ .

Hope this helps,
Chris

----------- Start Original Message -----------
: we are researching methods to inspect and determine the degree of corrosion based upon remaining wall thickness of about 40 cast and ductile iron water and wastewater subaqueous crossings in Pinellas County Florida USA.
: We are aware of Hydroscope and their service. Is there a competitor to Hydroscope in the marketplace?
: Thanks,
: Dana
------------ End Original Message ------------




    
 
 Reply 
 
Dan Cook, President of Hydroscope Inc., USA
Dan Cook, President of Hydroscope Inc., USA
01:14 Aug-13-2004
Re: RFEC Inspection of Cast and Ductile Iron Mains
----------- Start Original Message -----------
: Dana,
: I'm not sure if they're still in the business or not but a company called TexTex out of PA did some RFEC work for us a few years ago, maybe they're worth a visit: http://www.testex-ndt.com/ .
: Hope this helps,
: Chris
: : we are researching methods to inspect and determine the degree of corrosion based upon remaining wall thickness of about 40 cast and ductile iron water and wastewater subaqueous crossings in Pinellas County Florida USA.
: : We are aware of Hydroscope and their service. Is there a competitor to Hydroscope in the marketplace?
: : Thanks,
: : Dana
------------ End Original Message ------------
Dana and Chris:
We're alive and well. In the past we were made aware of a Company referred to as TexTex. We were told about the Company and we believe they have knowingly infringed upon our patents. TexTex was put on notice of the infringement by our lawyers. Please let us know if they are continuing to offer RFEC services. To understand our USPTO suite of issued and owned patent coverage, please call (505) 345-1897 or search www.uspto.gov


    
 
 Reply 
 

Product Spotlight

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

Aerospace Systems - Automated Ultrasonic Inspection

USL are specialists in the design and manufacture of turnkey ultrasonic inspection systems for aer
...
ospace applications. From monolithic composites to complex honeycomb structures. This video shows just a few examples of what is possible, find out more at: www.ultrasonic-sciences.co.uk
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window