RFEC Inspection of Cast and Ductile Iron Mains

we are researching methods to inspect and determine the degree of corrosion based upon remaining wall thickness of about 40 cast and ductile iron water and wastewater subaqueous crossings in Pinellas County Florida USA.

We are aware of Hydroscope and their service. Is there a competitor to Hydroscope in the marketplace?

Thanks,

Dana


    
 
 
Chris Coughlin
Chris Coughlin
03:06 Mar-25-2004
Re: RFEC Inspection of Cast and Ductile Iron Mains
Dana,

I'm not sure if they're still in the business or not but a company called TexTex out of PA did some RFEC work for us a few years ago, maybe they're worth a visit: http://www.testex-ndt.com/ .

Hope this helps,
Chris

----------- Start Original Message -----------
: we are researching methods to inspect and determine the degree of corrosion based upon remaining wall thickness of about 40 cast and ductile iron water and wastewater subaqueous crossings in Pinellas County Florida USA.
: We are aware of Hydroscope and their service. Is there a competitor to Hydroscope in the marketplace?
: Thanks,
: Dana
------------ End Original Message ------------




    
 
 
Dan Cook, President of Hydroscope Inc., USA
Dan Cook, President of Hydroscope Inc., USA
01:14 Aug-13-2004
Re: RFEC Inspection of Cast and Ductile Iron Mains
----------- Start Original Message -----------
: Dana,
: I'm not sure if they're still in the business or not but a company called TexTex out of PA did some RFEC work for us a few years ago, maybe they're worth a visit: http://www.testex-ndt.com/ .
: Hope this helps,
: Chris
: : we are researching methods to inspect and determine the degree of corrosion based upon remaining wall thickness of about 40 cast and ductile iron water and wastewater subaqueous crossings in Pinellas County Florida USA.
: : We are aware of Hydroscope and their service. Is there a competitor to Hydroscope in the marketplace?
: : Thanks,
: : Dana
------------ End Original Message ------------
Dana and Chris:
We're alive and well. In the past we were made aware of a Company referred to as TexTex. We were told about the Company and we believe they have knowingly infringed upon our patents. TexTex was put on notice of the infringement by our lawyers. Please let us know if they are continuing to offer RFEC services. To understand our USPTO suite of issued and owned patent coverage, please call (505) 345-1897 or search www.uspto.gov


    
 
 

Product Spotlight

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

High-end Ultrasonic Flaw Detector with 32:128PR PAUT and 2-ch TOFD: SyncScan 2

SIUI’s newly launched SyncScan 2, is a high-end ultrasonic flaw detector with 32:128PR PAUT and
...
2-ch TOFD, which can maximize your efficiency for PA and TOFD. ● Support PA/TOFD/UT ● 32-ch PA is more suitable for inspection on extra-thick wall and high-attenuation material. ● 32-ch PA and 2-ch TOFD work simultaneously. ● Support PR mode for corrosion inspection.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window