Technical Discussions
James R. Johnson
NDT Inspector
International Engineering Group, USA, Joined Apr 2004, 1

James R. Johnson

NDT Inspector
International Engineering Group,
USA,
Joined Apr 2004
1
00:27 Apr-13-2004
Welding Failures Historically related to Arc Strikes and or Microfractures

Hello to All,
I'm trying to find 1) Earliest (Historically as well) Recorded Welding Failures, 2) Any and all failures related to or initiated by Arc strikes and subsequent related Microfractures. I have attempted using over 37 search engines and typed in every permutation possible with glaringly little results unless I wish to spend L180 P for an English Publication on Welding Failure Catastrophes or some other book which would be fine but time is the issue it's running out. I don't need a lot of just specifically 2 or 3 examples each any help in this aera is much appreciated. I'm hoping to finish my student paper for Student Night at the 4-21 meeting of our ASM Chapter and the stone wall of literal search engines and Failure Analysis Businesses filling the Net Pages doesn't help.
Thanks,
J. R. Johnson



 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
01:34 Apr-13-2004
Re: Welding Failures Historically related to Arc Strikes and or Microfractures
A typical common failure as a result of Arc Strikes is development of Amine SCC in Carbon Steel Materials in Amine Service. Arc Strikes act as initiation. If you can find a copy look up the old API Guide To Refinery Inspection Chapter II.

Defects and Failures In Pressure Vessels & Piping - Helmut Thielsch 1965 references failures back to 1941. You could also try the major welding Institute TWI in UK Edison Welding Institute in USA.


 
 Reply 
 
Daniel H. Rice
Consultant, Ultrasonic Evaluation of Resistance Spot Welding
Daniel H. Rice Consulting Services, USA, Joined Jan 2003, 10

Daniel H. Rice

Consultant, Ultrasonic Evaluation of Resistance Spot Welding
Daniel H. Rice Consulting Services,
USA,
Joined Jan 2003
10
00:32 Apr-16-2004
Re: Welding Failures Historically related to Arc Strikes and or Microfractures
----------- Start Original Message -----------
: Hello to All,
: I'm trying to find 1) Earliest (Historically as well) Recorded Welding Failures, 2) Any and all failures related to or initiated by Arc strikes and subsequent related Microfractures. I have attempted using over 37 search engines and typed in every permutation possible with glaringly little results unless I wish to spend L180 P for an English Publication on Welding Failure Catastrophes or some other book which would be fine but time is the issue it's running out. I don't need a lot of just specifically 2 or 3 examples each any help in this aera is much appreciated. I'm hoping to finish my student paper for Student Night at the 4-21 meeting of our ASM Chapter and the stone wall of literal search engines and Failure Analysis Businesses filling the Net Pages doesn't help.
: Thanks,
: J. R. Johnson
------------ End Original Message ------------

Look in the following places
Linclon handbook of arc welding (current edition)
Linde Second Edition of oxy-acetylene Handbook
also look for hot rolled armor plate, effects of SMAW arc strikes (same material). This might be a military document, for metalurgical data that is now declassifed and in the library of congress.
The US navy would have the oldest data and had instances in their welding saftey manuals.OSHA used to send flyers on these occurances in the 80's.



 
 Reply 
 

Product Spotlight

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Panther

M2M PANTHER is a phased-array equipment designed for both desktop and industrial applications, offer
...
ing unparalleled performance in a compact unit. It combines the speed required for industrial integrated Phased-Array Ultrasound (PAUT) solutions, with the most complete set of total focusing method (TFM) imaging techniques, making it the ultimate tool for R&D and procedure qualification.
>

GUL QSR1® Scanning

How do you measure pipe wall thickness without direct access to the area? QSR® Scanning - Guide Wav
...
e Quantitative Short Range Scanning.
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>