00:27 Apr-13-2004
Welding Failures Historically related to Arc Strikes and or Microfractures

Hello to All,
I'm trying to find 1) Earliest (Historically as well) Recorded Welding Failures, 2) Any and all failures related to or initiated by Arc strikes and subsequent related Microfractures. I have attempted using over 37 search engines and typed in every permutation possible with glaringly little results unless I wish to spend L180 P for an English Publication on Welding Failure Catastrophes or some other book which would be fine but time is the issue it's running out. I don't need a lot of just specifically 2 or 3 examples each any help in this aera is much appreciated. I'm hoping to finish my student paper for Student Night at the 4-21 meeting of our ASM Chapter and the stone wall of literal search engines and Failure Analysis Businesses filling the Net Pages doesn't help.
Thanks,
J. R. Johnson



 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
01:34 Apr-13-2004
Re: Welding Failures Historically related to Arc Strikes and or Microfractures
A typical common failure as a result of Arc Strikes is development of Amine SCC in Carbon Steel Materials in Amine Service. Arc Strikes act as initiation. If you can find a copy look up the old API Guide To Refinery Inspection Chapter II.

Defects and Failures In Pressure Vessels & Piping - Helmut Thielsch 1965 references failures back to 1941. You could also try the major welding Institute TWI in UK Edison Welding Institute in USA.


 
 Reply 
 
Daniel H. Rice
Consultant, Ultrasonic Evaluation of Resistance Spot Welding
Daniel H. Rice Consulting Services, USA, Joined Jan 2003, 10

Daniel H. Rice

Consultant, Ultrasonic Evaluation of Resistance Spot Welding
Daniel H. Rice Consulting Services,
USA,
Joined Jan 2003
10
00:32 Apr-16-2004
Re: Welding Failures Historically related to Arc Strikes and or Microfractures
----------- Start Original Message -----------
: Hello to All,
: I'm trying to find 1) Earliest (Historically as well) Recorded Welding Failures, 2) Any and all failures related to or initiated by Arc strikes and subsequent related Microfractures. I have attempted using over 37 search engines and typed in every permutation possible with glaringly little results unless I wish to spend L180 P for an English Publication on Welding Failure Catastrophes or some other book which would be fine but time is the issue it's running out. I don't need a lot of just specifically 2 or 3 examples each any help in this aera is much appreciated. I'm hoping to finish my student paper for Student Night at the 4-21 meeting of our ASM Chapter and the stone wall of literal search engines and Failure Analysis Businesses filling the Net Pages doesn't help.
: Thanks,
: J. R. Johnson
------------ End Original Message ------------

Look in the following places
Linclon handbook of arc welding (current edition)
Linde Second Edition of oxy-acetylene Handbook
also look for hot rolled armor plate, effects of SMAW arc strikes (same material). This might be a military document, for metalurgical data that is now declassifed and in the library of congress.
The US navy would have the oldest data and had instances in their welding saftey manuals.OSHA used to send flyers on these occurances in the 80's.



 
 Reply 
 

Product Spotlight

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

GUL QSR1® Scanning

How do you measure pipe wall thickness without direct access to the area? QSR® Scanning - Guide Wav
...
e Quantitative Short Range Scanning.
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

Echomac® Small

Available with up to eight channels of electronics to detect and evaluate thickness, flaws and eccen
...
tricity, this UT tester is housed in a convenient, smaller cabinet. This instrument can be used in conjunction with bubbler or immersion tank systems, or with a test bench or in laboratory applications. The Echomac® Small is available in the FD4, FD6 or FD6A versions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window