Tariq
NDT Inspector,
Association sonatrach & British Petroleum & Statoil, Algeria, Joined Jun 2014, 10

Tariq

NDT Inspector,
Association sonatrach & British Petroleum & Statoil,
Algeria,
Joined Jun 2014
10
15:00 Jan-18-2017
The impact of removing excess welding metal

Hello Gents

In order to be able to have Ultrasonic reading of weld thickness over a nozzle, we removed the the Excess weld metal without touching the parent metal to have a straight contact between the UT probe and the weld metal
Question: is this removing of Excess weld metal affect negatively the integrity of equipment being tested or not

Thanks for advice me
Regards

 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1304

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1304
15:24 Jan-18-2017
Re: The impact of removing excess welding metal
In Reply to Tariq at 15:00 Jan-18-2017 (Opening).

Tariq, blending the excess weld cap metal to the parent metal is generally considered an improvement of the situation. Any stress riser effect at the transition is then removed. In some structures you will even find that the engineering drawings "require" removal of excess weld metal when the component is subject to cyclic loading.

 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
02:32 Jan-20-2017
Re: The impact of removing excess welding metal
In Reply to Tariq at 15:00 Jan-18-2017 (Opening).

Reinforcement is not intended to be part of the design thickness and in many codes is supposed to be removed to aide high quality NDE so your removal should not be an issue,

 
 Reply 
 
lawrence goldberg
NDT Inspector, NDT Inspector
USA, Joined May 2013, 13

lawrence goldberg

NDT Inspector, NDT Inspector
USA,
Joined May 2013
13
15:21 Jan-23-2017
Re: The impact of removing excess welding metal
In Reply to John O'Brien at 02:32 Jan-20-2017 .

One should look at AWS D1.1 and the usage of both weld toe grinding and weld toe hammer peening lg

 
 Reply 
 
Cesar Tovar
NDT Inspector, Quality assurance Representative
Toronto Transit Commission, Mexico, Joined Sep 2014, 7

Cesar Tovar

NDT Inspector, Quality assurance Representative
Toronto Transit Commission,
Mexico,
Joined Sep 2014
7
17:35 Jan-23-2017
Re: The impact of removing excess welding metal
In Reply to Tariq at 15:00 Jan-18-2017 (Opening).

Hi Tariq,

Here Engineering ordered do not touch the Crown in order to "increase" the life for a structure under cyclic load....the main issua is lack of penetration and lack of fusión at the root...and the results shows that the structure will have 30 years guaranty ...

 
 Reply 
 

Product Spotlight

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window