Cast Steel

I am trying to find an equivalent ISO and/or ASTM designations for BS 3100 Carbon & Manganese Casting Steels Grades AL1, AL2, AL3 & BL2.

Does anyone have any information on this or sources I can consult?


 
 Reply 
 
emily woo
emily woo
02:28 May-26-2004
Re: Cast Steel
i would like to know the advantages of CAST STEEL AS 2074 Grade C5.

----------- Start Original Message -----------
: I am trying to find an equivalent ISO and/or ASTM designations for BS 3100 Carbon & Manganese Casting Steels Grades AL1, AL2, AL3 & BL2.
: Does anyone have any information on this or sources I can consult?
------------ End Original Message ------------




 
 Reply 
 
James Dolfi
Director
ford, USA, Joined Oct 1999, 8

James Dolfi

Director
ford,
USA,
Joined Oct 1999
8
00:36 May-27-2004
Re: Cast Steel
----------- Start Original Message -----------
: i would like to know the advantages of CAST STEEL AS 2074 Grade C5.
: : I am trying to find an equivalent ISO and/or ASTM designations for BS 3100 Carbon & Manganese Casting Steels Grades AL1, AL2, AL3 & BL2.
: : Does anyone have any information on this or sources I can consult?
------------ End Original Message ------------

You may be able to get all the info you want at
http://www.key-to-steel.com/

They cross reference all steels and standards.



 
 Reply 
 
ian
ian
04:16 Jul-21-2004
Re: Cast Steel
thank you so much for this opportunity. i want to know about the chemical compositions of material called GS-60.3 . Thank you


 
 Reply 
 
Ed T.
Ed T.
05:28 Jul-22-2004
Re: Cast Steel
----------- Start Original Message -----------
: thank you so much for this opportunity. i want to know about the chemical compositions of material called GS-60.3 . Thank you
------------ End Original Message ------------
Try these links:

http://www.rz.fh-ulm.de/labore/wplabor/Englisch/FurtherInfo/Tests/Test11/metallographic%20determination%20v11.htm
http://www.felis.hr/en/cast-general.html
http://www.proximedia.com/local/jkservice/produkt1ban.htm


 
 Reply 
 

Product Spotlight

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window